Thermodynamic descriptions of ternary Al–Si–Yb system and their application to understand solidification behaviors of Yb-modified Al–Si alloys AITranslate
Abstract AITranslate
In this paper, thermodynamic descriptions of binary Si–Yb and ternary Al–Si-Yb system were assessed using the CALculation of PHAse Diagram (CALPHAD) technique, from which insights to the solidification behaviors of Yb-modified Al–Si alloys were attained. Firstly, all the experimental phase equilibria and thermodynamic properties in binary Si–Yb and ternary Al–Si-Yb systems were critically evaluated. Based on evaluated experimental data in the literature, the thermodynamic parameters of binary Si–Yb system were then updated, resulting in a better agreement with the experimental phase equilibrium data in Si-rich part than the previous assessment in the literature. Afterward, the thermodynamic descriptions of ternary Al–Si-Yb system were established on the basis of thermodynamic parameters of three boundary binaries, and their reliability was verified by comprehensively comparing the predicted thermodynamic properties/solidified behaviors with the literature data. Finally, the Scheil-Gulliver solidification simulations of different Yb-modified Al–Si alloys were conducted, from which the effect of Yb additions on the solidification sequences, phase transition temperatures, and phases/structures fractions in Al–Si-Yb alloys was analyzed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2023.102625
Chinese Library Classification Number:
Citation Information:
In this paper, thermodynamic descriptions of binary Si–Yb and ternary Al–Si-Yb system were assessed using the CALculation of PHAse Diagram (CALPHAD) technique, from which insights to the solidification behaviors of Yb-modified Al–Si alloys were attained. Firstly, all the experimental phase equilibria and thermodynamic properties in binary Si–Yb and ternary Al–Si-Yb systems were critically evaluated. Based on evaluated experimental data in the literature, the thermodynamic parameters of binary Si–Yb system were then updated, resulting in a better agreement with the experimental phase equilibrium data in Si-rich part than the previous assessment in the literature. Afterward, the thermodynamic descriptions of ternary Al–Si-Yb system were established on the basis of thermodynamic parameters of three boundary binaries, and their reliability was verified by comprehensively comparing the predicted thermodynamic properties/solidified behaviors with the literature data. Finally, the Scheil-Gulliver solidification simulations of different Yb-modified Al–Si alloys were conducted, from which the effect of Yb additions on the solidification sequences, phase transition temperatures, and phases/structures fractions in Al–Si-Yb alloys was analyzed.
quote
| GB/T 7714-2015 | [1] Mingzong Zhang, Jianbao Gao, Wang Yi, et al. Calphad, 2023(83). DOI:10.1016/j.calphad.2023.102625. |
| MLA | [1] Mingzong Zhang, et al., Calphad, no. 83, 2023, https://doi.org/10.1016/j.calphad.2023.102625. |
| APA | [1] Mingzong Zhang, Jianbao Gao, Wang Yi, Shenglan Yang, Shaoji Zhang, Zhao Lu, Enlang Feng, Liying Luo, & Lijun Zhang. (2023). Calphad(83). https://doi.org/10.1016/j.calphad.2023.102625 |