Rational Design of a Laminated Dual-Polymer/Polymer–Ceramic Composite Electrolyte for High-Voltage All-Solid-State Lithium Batteries AITranslate

The University of Texas at Austin; The University of Texas at Austin; The University of Texas at Austin
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We present a multi-layer approach to design a laminated dual-polymer/polymer–ceramic composite electrolyte (LDPPCCE) for high-voltage all-solid-state lithium batteries. An anode friendly poly(ethylene oxide) (PEO) serves as a matrix to face the Li-metal anode. To enhance the room-temperature Li+-ion conductivity, succinonitrile (SN) is incorporated into the PEO. At the cathode side, an oxidation tolerant poly(acrylonitrile) (PAN) matrix is employed. To enhance the ionic conductivity and suppress lithium dendrite, NASICON-type lithium aluminum titanium phosphate (Li1+xAlxTi2–x(PO4)3, LATP) powder is integrated into the PAN. The PEO-SN dual-polymer and the PAN-LATP composite deliver matched ionic conductivity. Uniting the two electrolyte layers, the resulting elastic LDPPCCE exhibits an ionic conductivity of 1.31 × 10–4 S cm–1 at ambient temperature with an electrochemical stability window of 0–5 V. All-solid-state lithium cells, fabricated with the LDPPCCE electrolyte, high-capacity/high-voltage LiNi0.8Co0.1Mn0.1O2 cathode, and lithium–metal anode exhibit exceptional electrochemical performance with a long cycle life.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.9b00535

Chinese Library Classification Number:

Citation Information:

We present a multi-layer approach to design a laminated dual-polymer/polymer–ceramic composite electrolyte (LDPPCCE) for high-voltage all-solid-state lithium batteries. An anode friendly poly(ethylene oxide) (PEO) serves as a matrix to face the Li-metal anode. To enhance the room-temperature Li+-ion conductivity, succinonitrile (SN) is incorporated into the PEO. At the cathode side, an oxidation tolerant poly(acrylonitrile) (PAN) matrix is employed. To enhance the ionic conductivity and suppress lithium dendrite, NASICON-type lithium aluminum titanium phosphate (Li1+xAlxTi2–x(PO4)3, LATP) powder is integrated into the PAN. The PEO-SN dual-polymer and the PAN-LATP composite deliver matched ionic conductivity. Uniting the two electrolyte layers, the resulting elastic LDPPCCE exhibits an ionic conductivity of 1.31 × 10–4 S cm–1 at ambient temperature with an electrochemical stability window of 0–5 V. All-solid-state lithium cells, fabricated with the LDPPCCE electrolyte, high-capacity/high-voltage LiNi0.8Co0.1Mn0.1O2 cathode, and lithium–metal anode exhibit exceptional electrochemical performance with a long cycle life.

quote

GB/T 7714-2015 [1] Xingwen Yu, Jianyu Li, Arumugam Manthiram. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.9b00535.
MLA [1] Xingwen Yu, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.9b00535.
APA [1] Xingwen Yu, Jianyu Li, & Arumugam Manthiram. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.9b00535
IEEE [1] Xingwen Yu, Jianyu Li, and Arumugam Manthiram, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.9b00535.