Tunable Actuation of Humidity-Driven Artificial Muscles via Graphene Nanofillers AITranslate

Texas A&M University; College Station; Texas A&M University; U.S. Army Combat Capabilities Development Command Army Research Laboratory; U.S. Army Combat Capabilities Development Command Army Research Laboratory; Texas A&M University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Humidity-responsive soft actuators can be driven by external stimuli and provide biomimetic environmental adaptations. Here, we report a humidity-responsive axial soft actuator of sulfonated polyether ether ketone which shows greatly tailorable actuation performance upon embedding graphene nanoplatelets (GNPs). Analysis of the experimental data shows that adding only 0.5 wt % GNP increases the actuation by 50% and provides a maximum actuation stroke of 24% and work capacity of 230 J/kg. In addition, 0.5 wt % GNP facilitates faster actuation, with significantly enhanced rates of both contraction and expansion. However, the addition of 1 wt % GNP slightly decreases the actuation magnitude. The nonmonotonic actuation performance was correlated with ion exchange capacity, water uptake, and GNP dispersion. By utilizing actuation magnitude tunability via GNP, the axial actuators were converted into a walking robot stacked of two active layers consisting of fibers of the same material system. The bilayer robot demonstrated self-crawling and locomotion ability in response to humidity changes. This study shows a uniquely tunable humidity actuator that demonstrates linear and bending actuation.

KeyWords AITranslate

soft actuators SPEEK graphene bilayer humiditydriven actuators walking robot
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01107

Chinese Library Classification Number:

Citation Information:

Humidity-responsive soft actuators can be driven by external stimuli and provide biomimetic environmental adaptations. Here, we report a humidity-responsive axial soft actuator of sulfonated polyether ether ketone which shows greatly tailorable actuation performance upon embedding graphene nanoplatelets (GNPs). Analysis of the experimental data shows that adding only 0.5 wt % GNP increases the actuation by 50% and provides a maximum actuation stroke of 24% and work capacity of 230 J/kg. In addition, 0.5 wt % GNP facilitates faster actuation, with significantly enhanced rates of both contraction and expansion. However, the addition of 1 wt % GNP slightly decreases the actuation magnitude. The nonmonotonic actuation performance was correlated with ion exchange capacity, water uptake, and GNP dispersion. By utilizing actuation magnitude tunability via GNP, the axial actuators were converted into a walking robot stacked of two active layers consisting of fibers of the same material system. The bilayer robot demonstrated self-crawling and locomotion ability in response to humidity changes. This study shows a uniquely tunable humidity actuator that demonstrates linear and bending actuation.

quote

GB/T 7714-2015 [1] Sevketcan Sarikaya, Frank Gardea, Hannah Strong, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01107.
MLA [1] Sevketcan Sarikaya, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01107.
APA [1] Sevketcan Sarikaya, Frank Gardea, Hannah Strong, Jeffrey T. Auletta, David M. Mackie, & Mohammad Naraghi. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01107
IEEE [1] Sevketcan Sarikaya, Frank Gardea, Hannah Strong, Jeffrey T. Auletta, David M. Mackie, and Mohammad Naraghi, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01107. keywords: {soft actuators;SPEEK;graphene;bilayer humiditydriven actuators;walking robot}