First-principles study of hydrogen storage and diffusion in B2 FeTi alloy AITranslate
Abstract AITranslate
Highlights • Hydrogen atom exists in octahedron with the frame of four Ti atoms and two Fe atoms. • FeTi and its hydrides all display small anisotropy in shear and compression. • Next nearest neighbor diffusion of H between octahedron interstices is the most likely diffusion mechanism. • Hydrogen diffusion is more difficult to occur in B2 FeTi alloy than that in β-Ti. The structural, elastic properties and electronic structure of FeTi and its hydrides, and hydrogen diffusion behavior in FeTi alloy were investigated by the first-principles calculations within the frame work of density functional theory (DFT). The calculated lattice constants for FeTi were in good agreement with the experimental values, and the lattice distortion of hydrides increases with the rise of hydrogen content. The calculation results of formation enthalpy, fusion heat of hydrogen and octahedron interstice size showed that hydrogen atom is more likely to exist in the central site of octahedron with the frame of four Ti atoms and two Fe atoms. The independent elastic constants as well as polycrystalline elastic parameters (bulk modulus B, shear modulus G, Young’s modulus E, Poisson’s ratio ν and anisotropy value A) were calculated, and then the ductility and elastic anisotropy of FeTi and its hydrides were discussed in details. In addition, the density of states, electron density difference and population analysis for FeTi and its hydrides were also calculated, which reveals the underlying mechanism of structural stability and chemical bonding. Finally, the activation energy of next nearest neighbor diffusion for H between octahedron interstices in FeTi alloy was calculated to be 2.92 eV, clarifying the atomic mechanism of hydrogen diffusion. Graphical abstract Download : Download high-res image (90KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2013.08.060
Chinese Library Classification Number:
Citation Information:
Highlights • Hydrogen atom exists in octahedron with the frame of four Ti atoms and two Fe atoms. • FeTi and its hydrides all display small anisotropy in shear and compression. • Next nearest neighbor diffusion of H between octahedron interstices is the most likely diffusion mechanism. • Hydrogen diffusion is more difficult to occur in B2 FeTi alloy than that in β-Ti. The structural, elastic properties and electronic structure of FeTi and its hydrides, and hydrogen diffusion behavior in FeTi alloy were investigated by the first-principles calculations within the frame work of density functional theory (DFT). The calculated lattice constants for FeTi were in good agreement with the experimental values, and the lattice distortion of hydrides increases with the rise of hydrogen content. The calculation results of formation enthalpy, fusion heat of hydrogen and octahedron interstice size showed that hydrogen atom is more likely to exist in the central site of octahedron with the frame of four Ti atoms and two Fe atoms. The independent elastic constants as well as polycrystalline elastic parameters (bulk modulus B, shear modulus G, Young’s modulus E, Poisson’s ratio ν and anisotropy value A) were calculated, and then the ductility and elastic anisotropy of FeTi and its hydrides were discussed in details. In addition, the density of states, electron density difference and population analysis for FeTi and its hydrides were also calculated, which reveals the underlying mechanism of structural stability and chemical bonding. Finally, the activation energy of next nearest neighbor diffusion for H between octahedron interstices in FeTi alloy was calculated to be 2.92 eV, clarifying the atomic mechanism of hydrogen diffusion. Graphical abstract Download : Download high-res image (90KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] ZhiSheng Nong, JingChuan Zhu, XiaWei Yang, et al. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.08.060. |
| MLA | [1] ZhiSheng Nong, et al., Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.08.060. |
| APA | [1] ZhiSheng Nong, JingChuan Zhu, XiaWei Yang, Yong Cao, ZhongHong Lai, & Yong Liu. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.08.060 |
| IEEE | [1] ZhiSheng Nong, JingChuan Zhu, XiaWei Yang, Yong Cao, ZhongHong Lai, and Yong Liu, Computational Materials Science, no. 81, 2014, doi: 10.1016/j.commatsci.2013.08.060. |