Observation of an Internal p–n Junction in Pyrite FeS2 Single Crystals: Potential Origin of the Low Open Circuit Voltage in Pyrite Solar Cells AITranslate

University of Minnesota; University of Minnesota; University of Minnesota; Augsburg University; University of Minnesota; University of Minnesota; University of Minnesota; New York University Tandon School of Engineering
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Pyrite FeS2 has long been considered a potentially ideal photovoltaic material, but solar cells utilizing pyrite exhibit low open-circuit voltages (VOC) and have failed to achieve conversion efficiencies >3%. The recent discovery of a conductive p-type surface layer on n-type pyrite single crystals raises the intriguing possibility that the low VOC results from a leaky internal p–n junction between the surface and interior. Here, we reveal this internal junction, for the first time, through horizontal electronic transport measurements on sulfur vacancy (VS)- and Co-doped n-type pyrite single crystals. We observe a steep increase in resistance upon cooling heavily VS-doped crystals below ∼200 K, as the dominant charge transport crosses over from interior to surface conduction. The frequently employed two-resistor equivalent circuit model for lightly-doped pyrite crystals cannot reproduce this steep rise, but it can be accounted for, quantitatively, and with high fidelity, by adding an internal Schottky junction resistance between the surface and the interior. The average extracted Schottky barrier height is 320 meV (varying from 130–560 meV), significantly below expectations from band bending calculations (>750 meV) but similar in magnitude to VOC values reported for pyrite heterojunction solar cells. This internal p–n junction is thus implicated as the potential origin of the long-standing low-VOC problem in pyrite.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00207

Chinese Library Classification Number:

Citation Information:

Pyrite FeS2 has long been considered a potentially ideal photovoltaic material, but solar cells utilizing pyrite exhibit low open-circuit voltages (VOC) and have failed to achieve conversion efficiencies >3%. The recent discovery of a conductive p-type surface layer on n-type pyrite single crystals raises the intriguing possibility that the low VOC results from a leaky internal p–n junction between the surface and interior. Here, we reveal this internal junction, for the first time, through horizontal electronic transport measurements on sulfur vacancy (VS)- and Co-doped n-type pyrite single crystals. We observe a steep increase in resistance upon cooling heavily VS-doped crystals below ∼200 K, as the dominant charge transport crosses over from interior to surface conduction. The frequently employed two-resistor equivalent circuit model for lightly-doped pyrite crystals cannot reproduce this steep rise, but it can be accounted for, quantitatively, and with high fidelity, by adding an internal Schottky junction resistance between the surface and the interior. The average extracted Schottky barrier height is 320 meV (varying from 130–560 meV), significantly below expectations from band bending calculations (>750 meV) but similar in magnitude to VOC values reported for pyrite heterojunction solar cells. This internal p–n junction is thus implicated as the potential origin of the long-standing low-VOC problem in pyrite.

quote

GB/T 7714-2015 [1] Bryan Voigt, William Moore, Moumita Maiti, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00207.
MLA [1] Bryan Voigt, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00207.
APA [1] Bryan Voigt, William Moore, Moumita Maiti, Jeff Walter, Bhaskar Das, Michael Manno, Chris Leighton, & Eray S. Aydil. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00207
IEEE [1] Bryan Voigt, William Moore, Moumita Maiti, Jeff Walter, Bhaskar Das, Michael Manno, Chris Leighton, and Eray S. Aydil, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00207.