An Interlayer Spacing-Anion Matching Guideline for High-Performance N-Doped Porous Carbon Cathode AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; City University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium-ion capacitors (LICs), by integrating the merits of batteries and supercapacitors, can improve energy/power density compatibly. However, the current understanding of the structure–property–performance relationship has limited the further development of carbon-based electrodes. Here we discuss how the architecture of interlayer channels influences the ion accessibility and selectivity in N-doped porous carbon (NDPC) cathodes. Electrochemical and spectroscopic measurements reveal that large interlayer channels provide high permeability for different anions and rearrange to buffer the volume variation. Conversely, narrow slits show high ion selectivity and suffer from distortion interacting with large anions. The turning point is the tuned channel size after the carbon layer rearrangement in the soaking process. Contrary to the popular opinion that pore size dominates capacitive behavior while d-spacing determines the intercalative process, we demonstrate the importance of interlayer spacing in electrical double-layer mechanism for NDPCs. This size effect is also successfully put into practice for developing advanced LICs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00924

Chinese Library Classification Number:

Citation Information:

Lithium-ion capacitors (LICs), by integrating the merits of batteries and supercapacitors, can improve energy/power density compatibly. However, the current understanding of the structure–property–performance relationship has limited the further development of carbon-based electrodes. Here we discuss how the architecture of interlayer channels influences the ion accessibility and selectivity in N-doped porous carbon (NDPC) cathodes. Electrochemical and spectroscopic measurements reveal that large interlayer channels provide high permeability for different anions and rearrange to buffer the volume variation. Conversely, narrow slits show high ion selectivity and suffer from distortion interacting with large anions. The turning point is the tuned channel size after the carbon layer rearrangement in the soaking process. Contrary to the popular opinion that pore size dominates capacitive behavior while d-spacing determines the intercalative process, we demonstrate the importance of interlayer spacing in electrical double-layer mechanism for NDPCs. This size effect is also successfully put into practice for developing advanced LICs.

quote

GB/T 7714-2015 [1] Kexin Liang, Kaixiang Zou, Jinhai Liu, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00924.
MLA [1] Kexin Liang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00924.
APA [1] Kexin Liang, Kaixiang Zou, Jinhai Liu, Yuanfu Deng, & Guohua Chen. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00924
IEEE [1] Kexin Liang, Kaixiang Zou, Jinhai Liu, Yuanfu Deng, and Guohua Chen, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00924.