daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Li+ Transport in Ethylene Carbonate Based Comb-Branched Solid Polymer Electrolyte: A Molecular Dynamics Simulation Study AITranslate

University of Utah; University of Utah; University of Utah
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid polymer electrolytes (SPEs) have the potential to resolve safety issues, be compatible with high-voltage cathode materials, and allow flexible designs of Li-ion batteries. Due to the limited Li+ transference number, a high degree of crystallinity at room temperature, and instability toward oxidation, polyether-based SPEs have been limited in batteries with the high-voltage cathodes and Li-metal anodes. Low ionic conductivity remains one of the biggest challenges for all types of SPE. Furthermore, the understanding of Li+ transport mechanisms and the related correlations with polymer structure are limited. In this study, extensive atomistic molecular dynamics simulations employing polarizable force field were conducted for a series of poly(alkyl ethylene carbonate) comb-branched architectures doped with lithium bis(trifluoromethane)sulfonimide salt. By studying systems with systematic variance in the polymer structure, the Li+ transport mechanisms have been investigated through structural and dynamical correlations of cation local environments. The molecular-scale insights into the Li+ transport allow proposing principles for the design of comb-branched SPEs with improved conductivity.

KeyWords AITranslate

solid polymer electrolyte combbranched polymer ethylene carbonate ion transport polymer relaxation molecular dynamics Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01416

Chinese Library Classification Number:

Citation Information:

Solid polymer electrolytes (SPEs) have the potential to resolve safety issues, be compatible with high-voltage cathode materials, and allow flexible designs of Li-ion batteries. Due to the limited Li+ transference number, a high degree of crystallinity at room temperature, and instability toward oxidation, polyether-based SPEs have been limited in batteries with the high-voltage cathodes and Li-metal anodes. Low ionic conductivity remains one of the biggest challenges for all types of SPE. Furthermore, the understanding of Li+ transport mechanisms and the related correlations with polymer structure are limited. In this study, extensive atomistic molecular dynamics simulations employing polarizable force field were conducted for a series of poly(alkyl ethylene carbonate) comb-branched architectures doped with lithium bis(trifluoromethane)sulfonimide salt. By studying systems with systematic variance in the polymer structure, the Li+ transport mechanisms have been investigated through structural and dynamical correlations of cation local environments. The molecular-scale insights into the Li+ transport allow proposing principles for the design of comb-branched SPEs with improved conductivity.

quote

GB/T 7714-2015 [1] Aditya Choudhary, Dengpan Dong, Dmitry Bedrov. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01416.
MLA [1] Aditya Choudhary, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01416.
APA [1] Aditya Choudhary, Dengpan Dong, & Dmitry Bedrov. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01416
IEEE [1] Aditya Choudhary, Dengpan Dong, and Dmitry Bedrov, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01416. keywords: {solid polymer electrolyte;combbranched polymer;ethylene carbonate;ion transport;polymer relaxation;molecular dynamics;Show More}