In Situ Spatially Coherent Identification of Phosphide-Based Catalysts: Crystallographic Latching for Highly Efficient Overall Water Electrolysis AITranslate

National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University; Taiwan|Japan Synchrotron Radiation Research Institute; Taiwan|Japan Synchrotron Radiation Research Institute; Taiwan|Japan Synchrotron Radiation Research Institute; National Taiwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Phosphide-based electrocatalysts exhibit high activities in alkaline solution toward overall water electrolysis. However, their real phases during catalysis have not been comprehensively identified, leading to improper advancement in material recognition and theoretical simulation. In this work, in situ spatially coherent transmitted X-ray diffraction and X-ray absorption spectroscopy were developed to probe Fe-doped cobalt phosphides, presenting superior catalytic activity and reaction kinetics for overall water electrolysis compared to pristine cobalt phosphides. The results showed that Fe dopants latched the crystallographic sites and stabilized the phosphide phase, which are the active species for hydrogen evolution reaction, while pristine cobalt phosphide transformed into hydroxides that impede the formation of active substances. Besides, Fe-doped cobalt phosphides swiftly converted into active-site confined oxyhydroxide for oxygen evolution reaction, achieving superb overall catalytic performance. The genuine materials unveiled during the electrocatalysis suggest that the appropriate catalytic mechanism correlates with the phase transition and crystalline transformation rate.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b02075

Chinese Library Classification Number:

Citation Information:

Phosphide-based electrocatalysts exhibit high activities in alkaline solution toward overall water electrolysis. However, their real phases during catalysis have not been comprehensively identified, leading to improper advancement in material recognition and theoretical simulation. In this work, in situ spatially coherent transmitted X-ray diffraction and X-ray absorption spectroscopy were developed to probe Fe-doped cobalt phosphides, presenting superior catalytic activity and reaction kinetics for overall water electrolysis compared to pristine cobalt phosphides. The results showed that Fe dopants latched the crystallographic sites and stabilized the phosphide phase, which are the active species for hydrogen evolution reaction, while pristine cobalt phosphide transformed into hydroxides that impede the formation of active substances. Besides, Fe-doped cobalt phosphides swiftly converted into active-site confined oxyhydroxide for oxygen evolution reaction, achieving superb overall catalytic performance. The genuine materials unveiled during the electrocatalysis suggest that the appropriate catalytic mechanism correlates with the phase transition and crystalline transformation rate.

quote

GB/T 7714-2015 [1] SungFu Hung, Yanping Zhu, GuanQuan Tzeng, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b02075.
MLA [1] SungFu Hung, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b02075.
APA [1] SungFu Hung, Yanping Zhu, GuanQuan Tzeng, HsiaoChien Chen, ChiaShuo Hsu, YenFa Liao, Hirofumi Ishii, Nozomu Hiraoka, & Hao Ming Chen. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b02075
IEEE [1] SungFu Hung, Yanping Zhu, GuanQuan Tzeng, HsiaoChien Chen, ChiaShuo Hsu, YenFa Liao, Hirofumi Ishii, Nozomu Hiraoka, and Hao Ming Chen, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b02075.