Beryllium doped graphene as an efficient anode material for lithium-ion batteries with significantly huge capacity: A DFT study AITranslate

Universidade Federal de Juiz de Fora;Computational Nanotechnology; Universidade Federal de Juiz de Fora
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

First-principles density functional theory (DFT) calculations were performed to investigate the lithium (Li) adsorption upon beryllium (Be) doped graphene. Be acts as hole doping in graphene leaving the structure as electron deficient, offering a greater tendency for Li adsorption than in pristine and boron (B) doped graphene. The introduction of Be augments the adsorption energy of Li from −1.11 to −2.53 eV/Li. Furthermore, 12, and 16 Li ions can easily be captured by one Be center in the single and double vacancy case, respectively, with the adsorption energies of −1.33 eV/Li (for both the cases), showing that Be doped graphene is an excellent anode material for lithium ion batteries (LIBs). Consequently, the presence of structural defects, in particular, a divacancy is found to be more efficient in terms of Li storage capacity. A huge Li storage capacity (2303.295 mAh/g) is calculated for Li8BeC7 having reasonable adsorption energy (−1.47 eV/Li). Our calculated capacity is 6.19 times greater than that of the graphite. Graphical abstract Be doped graphene is proposed for using as anode material in LIBs. The enhanced Li adsorption and huge storage capacity show that Be-graphene can be a best alternative to B-graphene.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2017.08.013

Chinese Library Classification Number:

Citation Information:

First-principles density functional theory (DFT) calculations were performed to investigate the lithium (Li) adsorption upon beryllium (Be) doped graphene. Be acts as hole doping in graphene leaving the structure as electron deficient, offering a greater tendency for Li adsorption than in pristine and boron (B) doped graphene. The introduction of Be augments the adsorption energy of Li from −1.11 to −2.53 eV/Li. Furthermore, 12, and 16 Li ions can easily be captured by one Be center in the single and double vacancy case, respectively, with the adsorption energies of −1.33 eV/Li (for both the cases), showing that Be doped graphene is an excellent anode material for lithium ion batteries (LIBs). Consequently, the presence of structural defects, in particular, a divacancy is found to be more efficient in terms of Li storage capacity. A huge Li storage capacity (2303.295 mAh/g) is calculated for Li8BeC7 having reasonable adsorption energy (−1.47 eV/Li). Our calculated capacity is 6.19 times greater than that of the graphite. Graphical abstract Be doped graphene is proposed for using as anode material in LIBs. The enhanced Li adsorption and huge storage capacity show that Be-graphene can be a best alternative to B-graphene.

quote

GB/T 7714-2015 [1] Saif Ullah, Pablo A. Denis, Fernando Sato. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.08.013.
MLA [1] Saif Ullah, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.08.013.
APA [1] Saif Ullah, Pablo A. Denis, & Fernando Sato. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.08.013
IEEE [1] Saif Ullah, Pablo A. Denis, and Fernando Sato, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.08.013.