daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Water Erosion Highly Recoverable and Flexible Photodetectors Based on Electrospun, Waterproof Perovskite–Polymer Fiber Membranes AITranslate

Shenzhen University; Shenzhen University; Shenzhen University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recently, there has been significant interest in perovskite–polymer composite nanostructures due to their biological nontoxicity and excellent waterproof stability. However, the exploration of their potential in water erosion highly recoverable and flexible high-performance photodetectors remains limited. In this study, we propose a specific photodetector (PD) strategy based on the electrospun perovskite–polymer [polymethyl methacrylate (PMMA)] fiber membranes (PPFMs), where perovskite nanocrystals are uniformly embedded within the long PMMA microfibers. The Schottky contact PDs, formed by in situ growth of PPFMs on lateral electrodes, exhibit ∼97% recovery in performance after drying the devices from the water-induced short-circuit states. The capacitive contact PDs, achieved by dry transfer of PPFMs onto the electrodes, maintain stable photoresponse with less than 2-fold performance fluctuations upon exposure to water, thanks to the suppressed water infiltration effects. Furthermore, due to the strong self-adhesion and flexibility of electrospun PPFMs, which establish tight contact with the lateral electrodes without requiring additional treatments, the PDs retain almost 100% of their original performances even after undergoing 500 bending cycles to a folded state.

KeyWords AITranslate

perovskite−polymer fiber membranes lateral photodetectors waterproof selfadhesive flexibility capillarity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00800

Chinese Library Classification Number:

Citation Information:

Recently, there has been significant interest in perovskite–polymer composite nanostructures due to their biological nontoxicity and excellent waterproof stability. However, the exploration of their potential in water erosion highly recoverable and flexible high-performance photodetectors remains limited. In this study, we propose a specific photodetector (PD) strategy based on the electrospun perovskite–polymer [polymethyl methacrylate (PMMA)] fiber membranes (PPFMs), where perovskite nanocrystals are uniformly embedded within the long PMMA microfibers. The Schottky contact PDs, formed by in situ growth of PPFMs on lateral electrodes, exhibit ∼97% recovery in performance after drying the devices from the water-induced short-circuit states. The capacitive contact PDs, achieved by dry transfer of PPFMs onto the electrodes, maintain stable photoresponse with less than 2-fold performance fluctuations upon exposure to water, thanks to the suppressed water infiltration effects. Furthermore, due to the strong self-adhesion and flexibility of electrospun PPFMs, which establish tight contact with the lateral electrodes without requiring additional treatments, the PDs retain almost 100% of their original performances even after undergoing 500 bending cycles to a folded state.

quote

GB/T 7714-2015 [1] Ying Chen, Zhen Yu Zhang, Guo Ping Wang. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00800.
MLA [1] Ying Chen, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00800.
APA [1] Ying Chen, Zhen Yu Zhang, & Guo Ping Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00800
IEEE [1] Ying Chen, Zhen Yu Zhang, and Guo Ping Wang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00800. keywords: {perovskite−polymer fiber membranes;lateral photodetectors;waterproof;selfadhesive flexibility;capillarity}