daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Solvation Structure of Conjugated Organosulfur Polymers for Lithium–Sulfur Battery Cathodes AITranslate

Applied Theoretical Physics − Computational Physics, Physikalisches Institut; Institute of Chemistry and Biochemistry;Applied Theoretical Physics − Computational Physics, Physikalisches Institut;Applied Theoretical Physics − Computational Physics, Physikalisches Institut
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium–sulfur (Li/S) batteries constitute a promising, next-generation energy storage technology due to their high theoretical energy density and low cost. To increase sustainability, processability, and battery performance, conducting organic polymers have become a focus of research for the development of better cathode materials. Here, we investigate the solvation structure of a single conjugated poly(4-(thiophen-3-yl)benzenethiol) (PTBT) polymer as a high-potential macromolecular candidate for synthesizing optimized cathodes in Li/S batteries. Using molecular dynamics (MD) simulation with newly optimized force-field parameters, we examine the effects of polymer length and various molar fractions of the popular dimethoxyethane (DME) and dioxolane (DOL) solvents on the structure of the PTBT polymer at a temperature of 300 K. We characterize basic polymeric properties as well as the composition-dependent solvent adsorption structure and thermodynamics and uncover significant tunability by the solvent. Importantly, we find an interesting cosolvency effect, namely that a solvent mixture composed of 25% DME and 75% DOL leads to maximum swelling behavior, which should be important for optimizing cathode fractality and permeability in applications. Our study thus reveals intriguing polymer–solvent correlations and serves as an important prerequisite for future MD studies of realistic polymeric cathode structures and processes, e.g., toward charge transport in vulcanized (S-linked) network topologies.

KeyWords AITranslate

Solvent quality cosolvency effect conjugated polymer polymer cathode molecular dynamics simulations forcefield development Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00379

Chinese Library Classification Number:

Citation Information:

Lithium–sulfur (Li/S) batteries constitute a promising, next-generation energy storage technology due to their high theoretical energy density and low cost. To increase sustainability, processability, and battery performance, conducting organic polymers have become a focus of research for the development of better cathode materials. Here, we investigate the solvation structure of a single conjugated poly(4-(thiophen-3-yl)benzenethiol) (PTBT) polymer as a high-potential macromolecular candidate for synthesizing optimized cathodes in Li/S batteries. Using molecular dynamics (MD) simulation with newly optimized force-field parameters, we examine the effects of polymer length and various molar fractions of the popular dimethoxyethane (DME) and dioxolane (DOL) solvents on the structure of the PTBT polymer at a temperature of 300 K. We characterize basic polymeric properties as well as the composition-dependent solvent adsorption structure and thermodynamics and uncover significant tunability by the solvent. Importantly, we find an interesting cosolvency effect, namely that a solvent mixture composed of 25% DME and 75% DOL leads to maximum swelling behavior, which should be important for optimizing cathode fractality and permeability in applications. Our study thus reveals intriguing polymer–solvent correlations and serves as an important prerequisite for future MD studies of realistic polymeric cathode structures and processes, e.g., toward charge transport in vulcanized (S-linked) network topologies.

quote

GB/T 7714-2015 [1] Diptesh Gayen, Yannik Schütze, Sebastien Groh, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00379.
MLA [1] Diptesh Gayen, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00379.
APA [1] Diptesh Gayen, Yannik Schütze, Sebastien Groh, & Joachim Dzubiella. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00379
IEEE [1] Diptesh Gayen, Yannik Schütze, Sebastien Groh, and Joachim Dzubiella, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00379. keywords: {Solvent quality;cosolvency effect;conjugated polymer;polymer cathode;molecular dynamics simulations;forcefield development;Show More}