Transforming Two-Dimensional Boron Carbide into Boron and Chlorine Dual-Doped Carbon Nanotubes by Chlorination for Efficient Oxygen Reduction AITranslate

Wuhan University of Technology; Wuhan University of Technology; Wuhan University of Technology; Wuhan University of Technology; Wuhan University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Our theoretical calculations suggest that the synergistic effect between the electron acceptor (B) and donor (Cl) in carbon nanotubes (CNTs) (BClCNTs) is the key to excellent oxygen reduction reaction (ORR) activity. However, the rational fabrication of BClCNTs is still an open question. Here, we first present a metal-free and controlled strategy for successful preparation of BClCNTs via chemically tailoring two-dimensional (2D) boron carbide (B4C) with Cl2. Accompanied by partial extraction of B atoms from B4C with Cl2, the residue B and C atoms combining with Cl atoms self-organize into nanotube microstructures. Significantly, the amount of heteroatoms (B and Cl) can be tuned in terms of altering chlorine-to-carbide molar ratios. As expected, as a metal-free ORR catalyst, the produced BClCNTs exhibit a higher onset potential (0.94 V vs a reversible hydrogen electrode; RHE) and half-wave potential (0.84 V) as well as greater stability than those of commercial Pt/C (0.92 and 0.80 V).

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01133

Chinese Library Classification Number:

Citation Information:

Our theoretical calculations suggest that the synergistic effect between the electron acceptor (B) and donor (Cl) in carbon nanotubes (CNTs) (BClCNTs) is the key to excellent oxygen reduction reaction (ORR) activity. However, the rational fabrication of BClCNTs is still an open question. Here, we first present a metal-free and controlled strategy for successful preparation of BClCNTs via chemically tailoring two-dimensional (2D) boron carbide (B4C) with Cl2. Accompanied by partial extraction of B atoms from B4C with Cl2, the residue B and C atoms combining with Cl atoms self-organize into nanotube microstructures. Significantly, the amount of heteroatoms (B and Cl) can be tuned in terms of altering chlorine-to-carbide molar ratios. As expected, as a metal-free ORR catalyst, the produced BClCNTs exhibit a higher onset potential (0.94 V vs a reversible hydrogen electrode; RHE) and half-wave potential (0.84 V) as well as greater stability than those of commercial Pt/C (0.92 and 0.80 V).

quote

GB/T 7714-2015 [1] Zongkui Kou, Beibei Guo, Daping He, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01133.
MLA [1] Zongkui Kou, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01133.
APA [1] Zongkui Kou, Beibei Guo, Daping He, Jian Zhang, & Shichun Mu. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01133
IEEE [1] Zongkui Kou, Beibei Guo, Daping He, Jian Zhang, and Shichun Mu, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01133.