Doping of Mesoscopic Charge Extraction Layers Enables the Design of Long-Time Stable Organic Solar Cells AITranslate

Institute of Materials for Electronics and Energy Technology (i-MEET);Institute of Materials for Electronics and Energy Technology (i-MEET);Physical Chemistry II and Interdisciplinary Center for Molecular Materials, Friedrich-Alexander-Universität Erlangen-Nürnberg;Institute of Materials for Electronics and Energy Technology (i-MEET);Physical Chemistry II and Interdisciplinary Center for Molecular Materials, Friedrich-Alexander-Universität Erlangen-Nürnberg; Germany|Helmholtz-Institute Erlangen-Nürnberg for Renewable Energy (HI ERN); Germany|Helmholtz-Institute Erlangen-Nürnberg for Renewable Energy (HI ERN)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Realizing efficient and stable organic solar cells (OSCs) via all-solution processing requires the design of tailored charge extraction interfaces. Herein, we demonstrate a substantially different interface concept for OSC that is based on a low-temperature processed mesoscopic hole transporting layer (HTL) derived from partially covered organic nanoparticles (NPs) in the n-i-p structure. The mesoscopic interface is further doped in a second coating step with an organic salt dopant, BCF-Li. The interactions among the dopant, the solvent for sequential doping, and the semiconductor layer are surprisingly complex. The mesoscopic interface is necessary to evenly wet the semiconductor and prevent the aggregation of the dopant. At the same time, the sequential process reduces the excess acceptor at the interface. Both processes together are necessary to generate an efficiently doped interface for low-Ohmic-charge extraction and stable contacts. Devices with fully solution-processed mesoscopic interfaces show a superb shelf lifetime of over 22000 h without encapsulation and a long-term operational stability under 1 sun illumination for 2000 h (T80). Flexible devices bypass 1000 bending cycles with negligible degradation. Mesoscopic doped interfaces are demonstrated as an alternative to PEDOT:PSS as well as PEDOT related interface concepts for nonfullerene acceptors (NFA) in the n-i-p architecture.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c02087

Chinese Library Classification Number:

Citation Information:

Realizing efficient and stable organic solar cells (OSCs) via all-solution processing requires the design of tailored charge extraction interfaces. Herein, we demonstrate a substantially different interface concept for OSC that is based on a low-temperature processed mesoscopic hole transporting layer (HTL) derived from partially covered organic nanoparticles (NPs) in the n-i-p structure. The mesoscopic interface is further doped in a second coating step with an organic salt dopant, BCF-Li. The interactions among the dopant, the solvent for sequential doping, and the semiconductor layer are surprisingly complex. The mesoscopic interface is necessary to evenly wet the semiconductor and prevent the aggregation of the dopant. At the same time, the sequential process reduces the excess acceptor at the interface. Both processes together are necessary to generate an efficiently doped interface for low-Ohmic-charge extraction and stable contacts. Devices with fully solution-processed mesoscopic interfaces show a superb shelf lifetime of over 22000 h without encapsulation and a long-term operational stability under 1 sun illumination for 2000 h (T80). Flexible devices bypass 1000 bending cycles with negligible degradation. Mesoscopic doped interfaces are demonstrated as an alternative to PEDOT:PSS as well as PEDOT related interface concepts for nonfullerene acceptors (NFA) in the n-i-p architecture.

quote

GB/T 7714-2015 [1] Junyi Xu, Junsheng Luo, Kirill Gubanov, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02087.
MLA [1] Junyi Xu, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02087.
APA [1] Junyi Xu, Junsheng Luo, Kirill Gubanov, Anastasiia Barabash, Rainer H. Fink, Thomas Heumüller, & Christoph J. Brabec. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02087
IEEE [1] Junyi Xu, Junsheng Luo, Kirill Gubanov, Anastasiia Barabash, Rainer H. Fink, Thomas Heumüller, and Christoph J. Brabec, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c02087.