daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fluorine Substitution at the O-Site Imparts Enhanced Chemical Stability for Garnet-Structured Electrolytes AITranslate

Jilin University; Jilin University; Jilin University;Key Laboratory of Neutron Physics and Institute of Nuclear Physics and Chemistry; Jilin University; Changchun Institute of Applied Chemistry; Jilin University; Jilin University; Jilin University; Jilin University; Jilin University; Jilin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Garnet-based superionic conductors hold great promise in next-generation lithium-ion batteries (LIBs) because of their favorable ionic conductivity and unique stability against Li-metal anodes; however, they still face the challenge of air stability for mass production/practical application. Herein, we identify their structural features and tailor the functional elements to enhance the chemical stability via synergistic control of doping and non-stoichiometry. The optimal composition of Li6.25Ga0.2La3Zr2O11.85F0.15 (LGLZO-0.15F) garnet exhibits great air durability without noticeable impurity accumulation, even during continuous air exposure for 60 days, owing to the high affinity of the fluorine dopant for lithium occupying the octahedral site. Meanwhile, LGLZO-0.15F possesses an appreciable Li-ion conductivity of 8.4 × 10–4 S cm–1 with an activation energy of 0.29 eV. Benefiting from these properties, hybrid and all-solid-state lithium batteries constructed with LGLZO-0.15F electrolytes demonstrate low overpotential, high Coulombic efficiency, and stable cycling performance.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02329

Chinese Library Classification Number:

Citation Information:

Garnet-based superionic conductors hold great promise in next-generation lithium-ion batteries (LIBs) because of their favorable ionic conductivity and unique stability against Li-metal anodes; however, they still face the challenge of air stability for mass production/practical application. Herein, we identify their structural features and tailor the functional elements to enhance the chemical stability via synergistic control of doping and non-stoichiometry. The optimal composition of Li6.25Ga0.2La3Zr2O11.85F0.15 (LGLZO-0.15F) garnet exhibits great air durability without noticeable impurity accumulation, even during continuous air exposure for 60 days, owing to the high affinity of the fluorine dopant for lithium occupying the octahedral site. Meanwhile, LGLZO-0.15F possesses an appreciable Li-ion conductivity of 8.4 × 10–4 S cm–1 with an activation energy of 0.29 eV. Benefiting from these properties, hybrid and all-solid-state lithium batteries constructed with LGLZO-0.15F electrolytes demonstrate low overpotential, high Coulombic efficiency, and stable cycling performance.

quote

GB/T 7714-2015 [1] Jingyu Shi, Ge Sun, Liping Li, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02329.
MLA [1] Jingyu Shi, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02329.
APA [1] Jingyu Shi, Ge Sun, Liping Li, Yuanhua Xia, Fei Du, Xiaojuan Liu, Hongwei Hou, Xiangyan Hou, Beining Zheng, Xiaofeng Wu, Keke Huang, & Shouhua Feng. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02329
IEEE [1] Jingyu Shi, Ge Sun, Liping Li, Yuanhua Xia, Fei Du, Xiaojuan Liu, Hongwei Hou, Xiangyan Hou, Beining Zheng, Xiaofeng Wu, Keke Huang, and Shouhua Feng, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02329.