Ultralarge Elastic Deformation (180° Fold) of Cubic-natBP Microwires for Wearable Flexible Strain Sensors AITranslate
Abstract AITranslate
Flexible strain sensors that can convert mechanical irritation from an external environment into electrical signals are key components in wearable devices. Here, using the principle of a B–Ni phase diagram, a pure-phase cubic natural boron phosphide (c-natBP) single-crystal microwire is obtained, which possesses ultralarge elastic deformation realized with the bending degree up to 180°. Based on the natBP microwire, a flexible strain sensor is prepared with an obvious quasi-linear response to external strain exhibited, which can be attributed to the Schottky barrier height (SBH) formed at the metal–crystal contact changing with the strain. Such strain-induced change results from lattice deformation, reconstructing the electronic structure and electron affinity. Furthermore, the effective and fast response of this flexible strain sensor in the practical applications of bicycle speed detection as well as finger and wrist bending detection demonstrates the potential of c-natBP microwire flexible strain sensors in wearable electronics, man–machine systems, and soft robotics.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c00454
Chinese Library Classification Number:
Citation Information:
Flexible strain sensors that can convert mechanical irritation from an external environment into electrical signals are key components in wearable devices. Here, using the principle of a B–Ni phase diagram, a pure-phase cubic natural boron phosphide (c-natBP) single-crystal microwire is obtained, which possesses ultralarge elastic deformation realized with the bending degree up to 180°. Based on the natBP microwire, a flexible strain sensor is prepared with an obvious quasi-linear response to external strain exhibited, which can be attributed to the Schottky barrier height (SBH) formed at the metal–crystal contact changing with the strain. Such strain-induced change results from lattice deformation, reconstructing the electronic structure and electron affinity. Furthermore, the effective and fast response of this flexible strain sensor in the practical applications of bicycle speed detection as well as finger and wrist bending detection demonstrates the potential of c-natBP microwire flexible strain sensors in wearable electronics, man–machine systems, and soft robotics.
quote
| GB/T 7714-2015 | [1] Xuefang Lu, Richeng Lin, Siqi Zhu, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00454. |
| MLA | [1] Xuefang Lu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00454. |
| APA | [1] Xuefang Lu, Richeng Lin, Siqi Zhu, Zhuogeng Lin, Xiaoyu Song, Feng Huang, & Wei Zheng. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00454 |
| IEEE | [1] Xuefang Lu, Richeng Lin, Siqi Zhu, Zhuogeng Lin, Xiaoyu Song, Feng Huang, and Wei Zheng, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00454. |