Insight into deformation allocation in the multi-pass roll forming of a double-walled brazed tube AITranslate
Abstract AITranslate
Deformation allocation is an important factor that affects 720° curling forming from copper-coated steel strips to double-walled brazed tubes (DWBTs). In this study, four schemes of deformation allocation, considering different weights of the total feed distance, are proposed, and a 3D finite element (FE) model of the multi-pass roll forming process for DWBT is developed and verified to investigate the cross-sectional evolution and deformation features. The results show the following. (i) In the 720° curling forming process from the steel strip into double-walled tubes, the curvature of the formed circular arc initially increases and then remains stable with roll forming, and the inner and outer tubes of the DWBT are formed in the third and fifth forming passes. Size forming can eliminate the gap between the double walls and improve the overall roundness. (ii) For different deformation allocations, the cross-sectional profiles of the roll-formed parts exhibit a discrepancy, and the deformation amount varies with the roll-forming process. The deformation amount in Scheme three is the maximum, and the cross-sectional profile deviates significantly from the ideal shape and fails to form a DWBT, which indicates that the deformation allocation is unsuitable. (iii) The roundness of the outer tube is better than that of the inner tube. Therefore, the roundness of the inner tube is the key to restricting the forming accuracy of the DWBT. Compared with Schemes one and two, Scheme four with a linear allocation of the total feed distance exhibits the best roundness, and the deformation allocation is reasonable; i.e., when the contact points between the rollers and steel strip are in a straight line, the roundness of the DWBT is in good agreement with the ideal condition.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1007/s40436-023-00448-y
Chinese Library Classification Number:
Citation Information:
Deformation allocation is an important factor that affects 720° curling forming from copper-coated steel strips to double-walled brazed tubes (DWBTs). In this study, four schemes of deformation allocation, considering different weights of the total feed distance, are proposed, and a 3D finite element (FE) model of the multi-pass roll forming process for DWBT is developed and verified to investigate the cross-sectional evolution and deformation features. The results show the following. (i) In the 720° curling forming process from the steel strip into double-walled tubes, the curvature of the formed circular arc initially increases and then remains stable with roll forming, and the inner and outer tubes of the DWBT are formed in the third and fifth forming passes. Size forming can eliminate the gap between the double walls and improve the overall roundness. (ii) For different deformation allocations, the cross-sectional profiles of the roll-formed parts exhibit a discrepancy, and the deformation amount varies with the roll-forming process. The deformation amount in Scheme three is the maximum, and the cross-sectional profile deviates significantly from the ideal shape and fails to form a DWBT, which indicates that the deformation allocation is unsuitable. (iii) The roundness of the outer tube is better than that of the inner tube. Therefore, the roundness of the inner tube is the key to restricting the forming accuracy of the DWBT. Compared with Schemes one and two, Scheme four with a linear allocation of the total feed distance exhibits the best roundness, and the deformation allocation is reasonable; i.e., when the contact points between the rollers and steel strip are in a straight line, the roundness of the DWBT is in good agreement with the ideal condition.
quote
| GB/T 7714-2015 | [1] MengMeng Liu, YuLi Liu, Heng Li. Advances in Manufacturing, 2023(11). DOI:10.1007/s40436-023-00448-y. |
| MLA | [1] MengMeng Liu, et al., Advances in Manufacturing, no. 11, 2023, https://doi.org/10.1007/s40436-023-00448-y. |
| APA | [1] MengMeng Liu, YuLi Liu, & Heng Li. (2023). Advances in Manufacturing(11). https://doi.org/10.1007/s40436-023-00448-y |
| IEEE | [1] MengMeng Liu, YuLi Liu, and Heng Li, Advances in Manufacturing, no. 11, 2023, doi: 10.1007/s40436-023-00448-y. keywords: {Doublewalled brazed tube (DWBT);Multipass roll forming;Deformation allocation;Crosssectional profile;Roundness} |