daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Efficient Synthesis of High-Molecular-Weight Biobased Polycarbonates by Lithium Lactate AITranslate

East China Normal University; East China Normal University; East China Normal University; East China Normal University; East China Normal University; Guangxi Normal University; East China Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Biobased polycarbonates have attracted a wide range of interest due to sustainable resources; however, the synthesis of biobased polycarbonates with a high molecular weight remains a great challenge on account of the influence of catalysts. Herein, biobased poly(isosorbide carbonate) (PIC) with a high molecular weight of 105.0 kDa and excellent light transparency was synthesized via melt polycondensation of isosorbide and diphenyl carbonate by an efficient lithium lactate catalyst under mild conditions, including a short transesterification time of 0.5 h at a low reaction temperature of 150 °C, followed by polycondensation at 200 °C for 1 h. Furthermore, the structures of reaction intermediates and polymers were characterized, and the catalytic mechanism was elucidated by density functional theory calculations. Such a low-cost commercial catalyst would have a broad application prospect in the industrial production of PIC.

KeyWords AITranslate

biobased polycarbonate melt polycondensation isosorbide diphenyl carbonate lithium lactate
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01463

Chinese Library Classification Number:

Citation Information:

Biobased polycarbonates have attracted a wide range of interest due to sustainable resources; however, the synthesis of biobased polycarbonates with a high molecular weight remains a great challenge on account of the influence of catalysts. Herein, biobased poly(isosorbide carbonate) (PIC) with a high molecular weight of 105.0 kDa and excellent light transparency was synthesized via melt polycondensation of isosorbide and diphenyl carbonate by an efficient lithium lactate catalyst under mild conditions, including a short transesterification time of 0.5 h at a low reaction temperature of 150 °C, followed by polycondensation at 200 °C for 1 h. Furthermore, the structures of reaction intermediates and polymers were characterized, and the catalytic mechanism was elucidated by density functional theory calculations. Such a low-cost commercial catalyst would have a broad application prospect in the industrial production of PIC.

quote

GB/T 7714-2015 [1] Tingting Wang, Qiubo Wang, Ying Quan, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01463.
MLA [1] Tingting Wang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01463.
APA [1] Tingting Wang, Qiubo Wang, Ying Quan, Xiaojuan Liao, Ruyi Sun, Liang Ding, & Meiran Xie. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01463
IEEE [1] Tingting Wang, Qiubo Wang, Ying Quan, Xiaojuan Liao, Ruyi Sun, Liang Ding, and Meiran Xie, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01463. keywords: {biobased polycarbonate;melt polycondensation;isosorbide;diphenyl carbonate;lithium lactate}