Abstract AITranslate

Polymeric biomaterials play a significant role in wound care. This article reviews the latest advances in polymeric biomaterials for the care of wound pathologies (i.e., chronic wounds and abnormal scarring). After discussing the development of three categories of polymers (i.e., biodegradable, stimuli-responsive, and bioinspired polymers), we focus on the prevention and treatment of abnormal scarring using polymeric biomaterials. Specific attention is paid to their roles in scar prevention, early detection of abnormal scarring, and antiscarring drug identification.

KeyWords AITranslate

wound healing pathological scarring skin polymer biomaterials
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00203

Chinese Library Classification Number:

Citation Information:

Polymeric biomaterials play a significant role in wound care. This article reviews the latest advances in polymeric biomaterials for the care of wound pathologies (i.e., chronic wounds and abnormal scarring). After discussing the development of three categories of polymers (i.e., biodegradable, stimuli-responsive, and bioinspired polymers), we focus on the prevention and treatment of abnormal scarring using polymeric biomaterials. Specific attention is paid to their roles in scar prevention, early detection of abnormal scarring, and antiscarring drug identification.

quote

GB/T 7714-2015 [1] David C. Yeo, Sharon W.T. Chew, Chenjie Xu. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00203.
MLA [1] David C. Yeo, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00203.
APA [1] David C. Yeo, Sharon W.T. Chew, & Chenjie Xu. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00203
IEEE [1] David C. Yeo, Sharon W.T. Chew, and Chenjie Xu, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00203. keywords: {wound healing;pathological scarring;skin;polymer;biomaterials}