Thermodynamic investigation of the galvanizing systems, I: Refinement of the thermodynamic description for the Fe–Zn system AITranslate

Central South University; Central South University; Central South University; University Park; Royal Institute of Technology; Central South University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The thermodynamic description for the Fe–Zn system was updated using CALPHAD approach. A set of self-consistent thermodynamic model parameters for this system was obtained by considering the available experimental data. Compared with the previous thermodynamic modeling, the present assessment with fewer parameters shows not only a better agreement with the experiments but also sounder physical meaning. The present CALPHAD modeling coupled with the ab initio calculations were used to predict the enthalpies of formation of the solid phases in the Fe–Zn system.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2009.01.002

Chinese Library Classification Number:

Citation Information:

The thermodynamic description for the Fe–Zn system was updated using CALPHAD approach. A set of self-consistent thermodynamic model parameters for this system was obtained by considering the available experimental data. Compared with the previous thermodynamic modeling, the present assessment with fewer parameters shows not only a better agreement with the experiments but also sounder physical meaning. The present CALPHAD modeling coupled with the ab initio calculations were used to predict the enthalpies of formation of the solid phases in the Fe–Zn system.

quote

GB/T 7714-2015 [1] Wei Xiong, Yi Kong, Yong Du, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.01.002.
MLA [1] Wei Xiong, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.01.002.