Recent enterprises in high-rate monolithic photo-electrochemical energy harvest and storage devices AITranslate

University Park; University Park; University Park; University Park
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solar energy is set to play a major role in decarbonising the economy and creating a zero-emissions future. However, there is a need to store this abundant energy and, in many instances, supply that energy at a high rate. With large expense and efficiency losses in integration through external circuits, a monolithic two-electrode harvest storage device or photo-supercapacitor with a high-power density and stable life cycles is an exciting challenge. Here we review the most recent advancements in photo-supercapacitors and some approaches to overcoming various challenges to delivering a marketable device. Graphical abstract Download : Download high-res image (293KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.coelec.2023.101243

Chinese Library Classification Number:

Citation Information:

Solar energy is set to play a major role in decarbonising the economy and creating a zero-emissions future. However, there is a need to store this abundant energy and, in many instances, supply that energy at a high rate. With large expense and efficiency losses in integration through external circuits, a monolithic two-electrode harvest storage device or photo-supercapacitor with a high-power density and stable life cycles is an exciting challenge. Here we review the most recent advancements in photo-supercapacitors and some approaches to overcoming various challenges to delivering a marketable device. Graphical abstract Download : Download high-res image (293KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Daniel Turner, Ming Li, David Grant, et al. Current Opinion in Electrochemistry, 2023(38). DOI:10.1016/j.coelec.2023.101243.
MLA [1] Daniel Turner, et al., Current Opinion in Electrochemistry, no. 38, 2023, https://doi.org/10.1016/j.coelec.2023.101243.
APA [1] Daniel Turner, Ming Li, David Grant, & Oluwafunmilola Ola. (2023). Current Opinion in Electrochemistry(38). https://doi.org/10.1016/j.coelec.2023.101243
IEEE [1] Daniel Turner, Ming Li, David Grant, and Oluwafunmilola Ola, Current Opinion in Electrochemistry, no. 38, 2023, doi: 10.1016/j.coelec.2023.101243.