daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Multiscale Polymer Dynamics in Hierarchical Carbon Nanotube Grafted Glass Fiber Reinforced Composites AITranslate

National Institute of Standards and Technology; Texas Tech University; Koç University; University of Delaware; University of Maryland; Georgetown University; National Institute of Standards and Technology; University of Delaware; National Institute of Standards and Technology; National Institute of Standards and Technology; National Institute of Standards and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Carbon nanotube (CNT) grafted glass fiber reinforced epoxy nanocomposites (GFRP) present a range of stiffnesses (MPa to GPa) and length scales (μm to nm) at the fiber–matrix interface. The contribution of functionalized CNT networks to the local and bulk polymer dynamics is studied here by using a combination of torsion dynamical mechanical thermal analysis (DMTA), positron annihilation lifetime spectroscopy (PALS), and neutron scattering (NS) measurements. DMTA measurements highlight a reduction in the storage modulus (G′) in the rubbery region and an asymmetric broadening of the loss modulus (G″) peak in the α-transition region. NS measurements show a suppressed hydrogen mean-square displacement (MSD) in the presence of glass fibers but a higher hydrogen MSD after grafting functionalized CNTs onto fiber surfaces. PALS measurements show greater free volume characteristics in the presence of the functionalized CNT modified composites, supporting the view that these interface layers increase polymer mobility. While NS and DMTA are sensitive to different modes of chain dynamics, the localization of functionalized nanotubes at the fiber interface is found to affect the distribution of polymer relaxation modes without significantly altering the thermally activated relaxation processes.

KeyWords AITranslate

carbon nanotube composites polymer nanocomposites fiber reinforced polymer nanocomposites polymer dynamics Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00464

Chinese Library Classification Number:

Citation Information:

Carbon nanotube (CNT) grafted glass fiber reinforced epoxy nanocomposites (GFRP) present a range of stiffnesses (MPa to GPa) and length scales (μm to nm) at the fiber–matrix interface. The contribution of functionalized CNT networks to the local and bulk polymer dynamics is studied here by using a combination of torsion dynamical mechanical thermal analysis (DMTA), positron annihilation lifetime spectroscopy (PALS), and neutron scattering (NS) measurements. DMTA measurements highlight a reduction in the storage modulus (G′) in the rubbery region and an asymmetric broadening of the loss modulus (G″) peak in the α-transition region. NS measurements show a suppressed hydrogen mean-square displacement (MSD) in the presence of glass fibers but a higher hydrogen MSD after grafting functionalized CNTs onto fiber surfaces. PALS measurements show greater free volume characteristics in the presence of the functionalized CNT modified composites, supporting the view that these interface layers increase polymer mobility. While NS and DMTA are sensitive to different modes of chain dynamics, the localization of functionalized nanotubes at the fiber interface is found to affect the distribution of polymer relaxation modes without significantly altering the thermally activated relaxation processes.

quote

GB/T 7714-2015 [1] Ajay Krishnamurthy, Ran Tao, Erkan Senses, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00464.
MLA [1] Ajay Krishnamurthy, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00464.
APA [1] Ajay Krishnamurthy, Ran Tao, Erkan Senses, Sagar M. Doshi, Faraz Ahmed Burni, Bharath Natarajan, Donald Hunston, Erik T. Thostenson, Antonio Faraone, Amanda L. Forster, & Aaron M. Forster. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00464
IEEE [1] Ajay Krishnamurthy, Ran Tao, Erkan Senses, Sagar M. Doshi, Faraz Ahmed Burni, Bharath Natarajan, Donald Hunston, Erik T. Thostenson, Antonio Faraone, Amanda L. Forster, and Aaron M. Forster, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00464. keywords: {carbon nanotube composites;polymer nanocomposites;fiber reinforced polymer nanocomposites;polymer dynamics;Show More}