Chrysin-Based Bio-Benzoxazine: A Copolymerizable Green Additive for Lowering Curing Temperatures and Improving Thermal Properties of Various Thermosetting Resins AITranslate
Abstract AITranslate
Adding copolymerizable components into thermosetting resins is a common strategy to improve the thermal and mechanical properties of thermosets. However, it remains quite challenging to discover a universal copolymerizable additive that is applicable for various thermosetting systems. Here, the flexible molecular design of benzoxazine allows us to design a biobased benzoxazine monomer (CHR-ac) with several smart functionalities, which can copolymerize with various traditional thermosetting systems, including benzoxazine, epoxy, and bismaleimide resins. CHR-ac has been synthesized using paraformaldehyde, 3-aminophenylacetylene, and natural renewable chrysin as raw materials via the Mannich condensation. Specifically, the built-in intramolecular hydrogen bonding in CHR-ac results in a low polymerization temperature while it still maintains the advantage of long shelf life. In addition, the phenolic hydroxyl and acetylene groups in CHR-ac enable it to cross-link with well-commercialized thermosetting resins and significantly enhance their performance through the formation of highly cross-linked networks. Potentially, the rationally designed biobased benzoxazine in the current work can be used as a generic additive in thermosetting resins for applications spanning from the microelectronic to the aerospace industries.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01679
Chinese Library Classification Number:
Citation Information:
Adding copolymerizable components into thermosetting resins is a common strategy to improve the thermal and mechanical properties of thermosets. However, it remains quite challenging to discover a universal copolymerizable additive that is applicable for various thermosetting systems. Here, the flexible molecular design of benzoxazine allows us to design a biobased benzoxazine monomer (CHR-ac) with several smart functionalities, which can copolymerize with various traditional thermosetting systems, including benzoxazine, epoxy, and bismaleimide resins. CHR-ac has been synthesized using paraformaldehyde, 3-aminophenylacetylene, and natural renewable chrysin as raw materials via the Mannich condensation. Specifically, the built-in intramolecular hydrogen bonding in CHR-ac results in a low polymerization temperature while it still maintains the advantage of long shelf life. In addition, the phenolic hydroxyl and acetylene groups in CHR-ac enable it to cross-link with well-commercialized thermosetting resins and significantly enhance their performance through the formation of highly cross-linked networks. Potentially, the rationally designed biobased benzoxazine in the current work can be used as a generic additive in thermosetting resins for applications spanning from the microelectronic to the aerospace industries.
quote
| GB/T 7714-2015 | [1] Boran Hao, Jiaqi Wang, Yuan Zhang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01679. |
| MLA | [1] Boran Hao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01679. |
| APA | [1] Boran Hao, Jiaqi Wang, Yuan Zhang, Weichen Sheng, & Kan Zhang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01679 |
| IEEE | [1] Boran Hao, Jiaqi Wang, Yuan Zhang, Weichen Sheng, and Kan Zhang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01679. keywords: {Benzoxazine;chrysin;natural renewable resources;green additive;low curing temperature;high performance;polybenzoxazine} |