Pyrazine-Based Covalent Organic Frameworks for Effective Iodine and Carbon Dioxide Capture AITranslate
Abstract AITranslate
Covalent organic frameworks (COFs) possess good porosity, uniform channels, and tunable skeletons, as well as excellent stability, which are well-suited for gas adsorption. In this study, we developed two pyrazine-based COFs, namely, TFPPz–MPA–COF and TFPPz–BD(OMe)2–COF, by condensation reaction of C4 and C2 axisymmetric monomers. Both COFs exhibited good crystallinity, well-defined pore structures, and outstanding thermal and chemical stability. TFPPz–MPA–COF and TFPPz–BD(OMe)2–COF demonstrated high iodine adsorption capabilities of up to 5.41 and 5.18 g g–1 in iodine vapor, and 95.42 and 98.04 mg g–1 in n-hexane, respectively. In addition, TFPPz–MPA–COF and TFPPz–BD(OMe)2–COF exhibited good CO2 uptake capacities of 1.48 and 1.34 mmol g–1 at 273 K, respectively.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01950
Chinese Library Classification Number:
Citation Information:
Covalent organic frameworks (COFs) possess good porosity, uniform channels, and tunable skeletons, as well as excellent stability, which are well-suited for gas adsorption. In this study, we developed two pyrazine-based COFs, namely, TFPPz–MPA–COF and TFPPz–BD(OMe)2–COF, by condensation reaction of C4 and C2 axisymmetric monomers. Both COFs exhibited good crystallinity, well-defined pore structures, and outstanding thermal and chemical stability. TFPPz–MPA–COF and TFPPz–BD(OMe)2–COF demonstrated high iodine adsorption capabilities of up to 5.41 and 5.18 g g–1 in iodine vapor, and 95.42 and 98.04 mg g–1 in n-hexane, respectively. In addition, TFPPz–MPA–COF and TFPPz–BD(OMe)2–COF exhibited good CO2 uptake capacities of 1.48 and 1.34 mmol g–1 at 273 K, respectively.
quote
| GB/T 7714-2015 | [1] Yamin He, YiFan Liu, Xinyu Shen, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01950. |
| MLA | [1] Yamin He, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01950. |
| APA | [1] Yamin He, YiFan Liu, Xinyu Shen, Jie Zhao, Lan Yang, & RuYi Zou. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01950 |
| IEEE | [1] Yamin He, YiFan Liu, Xinyu Shen, Jie Zhao, Lan Yang, and RuYi Zou, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01950. keywords: {covalent organic frameworks (COFs);iodine capture;iodine complex;CO2 adsorption;pyrazine core} |