Time-Domain ab Initio Analysis Rationalizes the Unusual Temperature Dependence of Charge Carrier Relaxation in Lead Halide Perovskite AITranslate

Hunan Agricultural University; Hunan Agricultural University;Donostia International Physics Center (DIPC), 20018 Donostia; University of Southern California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Increased charge carrier lifetimes at elevated temperatures constitute an intriguing and valuable feature of hybrid organic–inorganic perovskites that are subject to heating in solar energy applications. We rationalize this peculiar behavior at the atomistic level using real-time time-dependent density functional theory and nonadiabatic molecular dynamics. Focusing on tetragonal MAPbI3, we demonstrate that temperature has different effects on the organic and inorganic subsystems and leads to subtle structural changes, decreasing nonradiative electron–hole recombination. First, charge–phonon interactions are decreased because the libration dynamics of the organic component at higher temperature reduces the oscillation amplitude of the Pb–I lattice that supports electrons and holes. Second, thermal disorder localizes wave functions, reducing the nonadiabatic charge–phonon coupling. Third, tilting of the inorganic octahedra increases the bandgap, extending charge carrier lifetime further. The detailed time-domain atomistic analysis of the uncommon dependence of charge recombination on temperature emphasizes the key role played by the organic cation, establishes important structure–property relationships, provides valuable insights into efficient performance of perovskite solar cells, and highlights factors required to maintain and improve such performance.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01608

Chinese Library Classification Number:

Citation Information:

Increased charge carrier lifetimes at elevated temperatures constitute an intriguing and valuable feature of hybrid organic–inorganic perovskites that are subject to heating in solar energy applications. We rationalize this peculiar behavior at the atomistic level using real-time time-dependent density functional theory and nonadiabatic molecular dynamics. Focusing on tetragonal MAPbI3, we demonstrate that temperature has different effects on the organic and inorganic subsystems and leads to subtle structural changes, decreasing nonradiative electron–hole recombination. First, charge–phonon interactions are decreased because the libration dynamics of the organic component at higher temperature reduces the oscillation amplitude of the Pb–I lattice that supports electrons and holes. Second, thermal disorder localizes wave functions, reducing the nonadiabatic charge–phonon coupling. Third, tilting of the inorganic octahedra increases the bandgap, extending charge carrier lifetime further. The detailed time-domain atomistic analysis of the uncommon dependence of charge recombination on temperature emphasizes the key role played by the organic cation, establishes important structure–property relationships, provides valuable insights into efficient performance of perovskite solar cells, and highlights factors required to maintain and improve such performance.

quote

GB/T 7714-2015 [1] Wei Li, Jianfeng Tang, David Casanova, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01608.
MLA [1] Wei Li, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01608.
APA [1] Wei Li, Jianfeng Tang, David Casanova, & Oleg V. Prezhdo. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01608
IEEE [1] Wei Li, Jianfeng Tang, David Casanova, and Oleg V. Prezhdo, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01608.