Highly Sensitive Humidity Sensor Based on Ionic Liquid–Polymer Composites AITranslate

BCMaterials, Basque Center for Materials; University of Minho; University of Minho;BCMaterials, Basque Center for Materials;BCMaterials, Basque Center for Materials
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polymer composites comprising the ionic liquid (IL) [Bmim][FeCl4] and poly(vinylidene fluoride) (PVDF) have been developed for humidity sensing applications. Different IL contents (5, 10, and 20 wt %) were incorporated into the PVDF matrix and the morphological, physical–chemical and electrical properties of the composites evaluated, together with their humidity sensitivity response. Higher IL contents (20 wt %) induce a porous morphology in the composites. Further, IL incorporation leads to the crystallization of PVDF in the electroactive β phase, which content increases with the incorporation of IL into the polymer. The thermal stability of the composites decreases with increasing IL content. The humidity sensing response of the composites was evaluated with relative humidity variations from 35 to 90%. It is shown that all composites exhibit a linear resistance variation with the relative humidity, the sensitivity to humidity variations increasing linearly with the IL content. The developed materials show a strong potentiality for printable humidity sensors.

KeyWords AITranslate

ionic liquids electroactive materials multifunctional materials sensing materials humidity sensors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00675

Chinese Library Classification Number:

Citation Information:

Polymer composites comprising the ionic liquid (IL) [Bmim][FeCl4] and poly(vinylidene fluoride) (PVDF) have been developed for humidity sensing applications. Different IL contents (5, 10, and 20 wt %) were incorporated into the PVDF matrix and the morphological, physical–chemical and electrical properties of the composites evaluated, together with their humidity sensitivity response. Higher IL contents (20 wt %) induce a porous morphology in the composites. Further, IL incorporation leads to the crystallization of PVDF in the electroactive β phase, which content increases with the incorporation of IL into the polymer. The thermal stability of the composites decreases with increasing IL content. The humidity sensing response of the composites was evaluated with relative humidity variations from 35 to 90%. It is shown that all composites exhibit a linear resistance variation with the relative humidity, the sensitivity to humidity variations increasing linearly with the IL content. The developed materials show a strong potentiality for printable humidity sensors.

quote

GB/T 7714-2015 [1] L. C. Fernandes, D. M. Correia, N. Pereira, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00675.
MLA [1] L. C. Fernandes, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00675.
APA [1] L. C. Fernandes, D. M. Correia, N. Pereira, C. R. Tubio, & S. LancerosMéndez. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00675
IEEE [1] L. C. Fernandes, D. M. Correia, N. Pereira, C. R. Tubio, and S. LancerosMéndez, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00675. keywords: {ionic liquids;electroactive materials;multifunctional materials;sensing materials;humidity sensors}