Electrochemical Nitrogen Reduction Reaction on Ruthenium AITranslate
Abstract AITranslate
Ruthenium is a good catalyst for ammonia synthesis in the Haber–Bosch process and a promising electrocatalyst for electrochemical N2 reduction reaction (NRR). However, the NRR pathway on Ru is unclear because of the lack of information on reaction intermediates. Surface-enhanced infrared absorption spectroscopy combined with electrochemical measurements is employed to study the NRR mechanisms on Ru thin film. During the nitrogen reduction, the *N2Hx (0 ≤ x ≤ 2) was detected with the band of N=N stretching (∼1940 cm–1) at potentials below 0.2 V in an N2-satureated HClO4 solution. The coverage of *N2Hx on the Ru surface was significantly increased with the potential decreasing from 0.2 to −0.4 V. The formed *N2Hx species could be oxidized at potentials higher than −0.1 V. In an N2-satureated KOH solution, no N-related infrared absorption band was observed on Ru surfaces, indicating that the adsorption of nitrogen molecules on Ru surfaces is very weak.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00699
Chinese Library Classification Number:
Citation Information:
Ruthenium is a good catalyst for ammonia synthesis in the Haber–Bosch process and a promising electrocatalyst for electrochemical N2 reduction reaction (NRR). However, the NRR pathway on Ru is unclear because of the lack of information on reaction intermediates. Surface-enhanced infrared absorption spectroscopy combined with electrochemical measurements is employed to study the NRR mechanisms on Ru thin film. During the nitrogen reduction, the *N2Hx (0 ≤ x ≤ 2) was detected with the band of N=N stretching (∼1940 cm–1) at potentials below 0.2 V in an N2-satureated HClO4 solution. The coverage of *N2Hx on the Ru surface was significantly increased with the potential decreasing from 0.2 to −0.4 V. The formed *N2Hx species could be oxidized at potentials higher than −0.1 V. In an N2-satureated KOH solution, no N-related infrared absorption band was observed on Ru surfaces, indicating that the adsorption of nitrogen molecules on Ru surfaces is very weak.
quote
| GB/T 7714-2015 | [1] Yao Yao, Haijiang Wang, Xiaozi Yuan, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00699. |
| MLA | [1] Yao Yao, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00699. |
| APA | [1] Yao Yao, Haijiang Wang, Xiaozi Yuan, Hui Li, & Minhua Shao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00699 |
| IEEE | [1] Yao Yao, Haijiang Wang, Xiaozi Yuan, Hui Li, and Minhua Shao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00699. |