A-Site Cation Dependence of Self-Healing in Polycrystalline APbI3 Perovskite Films AITranslate

Weizmann Institute of Science; Weizmann Institute of Science;CNRS UMR 9006-IPVF Institut Photovoltaïque d’Ile-de-France, 18 Boulevard Thomas Gobert; Weizmann Institute of Science; Weizmann Institute of Science; Weizmann Institute of Science; Weizmann Institute of Science
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In terms of sustainable use, halide perovskite (HaP) semiconductors have a strong advantage over most other classes of materials for (opto)electronics, as they can self-heal (SH) from photodamage. While there is considerable literature on SH in devices, where it may not be clear exactly where damage and SH occur, there is much less on the HaP material itself. Here we perform “fluorescence recovery after photobleaching” (FRAP) measurements to study SH on polycrystalline thin films for which encapsulation is critical to achieving complete and fast self-healing. We compare SH in three photoactive APbI3 perovskite films by varying the A-site cation ranging from (relatively) small inorganic Cs through medium-sized MA to large FA (the last two are organic cations). While the A cation is often considered electronically relatively inactive, it significantly affects both SH kinetics and the threshold for photodamage. The SH kinetics are markedly faster for γ-CsPbI3 and α-FAPbI3 than for MAPbI3. Furthermore, γ-CsPbI3 exhibits an intricate interplay between photoinduced darkening and brightening. We suggest possible explanations for the observed differences in SH behavior. This study’s results are essential for identifying absorber materials that can regain intrinsic, insolation-induced photodamage-linked efficiency loss during its rest cycles, thus enabling applications such as autonomously sustainable electronics.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00017

Chinese Library Classification Number:

Citation Information:

In terms of sustainable use, halide perovskite (HaP) semiconductors have a strong advantage over most other classes of materials for (opto)electronics, as they can self-heal (SH) from photodamage. While there is considerable literature on SH in devices, where it may not be clear exactly where damage and SH occur, there is much less on the HaP material itself. Here we perform “fluorescence recovery after photobleaching” (FRAP) measurements to study SH on polycrystalline thin films for which encapsulation is critical to achieving complete and fast self-healing. We compare SH in three photoactive APbI3 perovskite films by varying the A-site cation ranging from (relatively) small inorganic Cs through medium-sized MA to large FA (the last two are organic cations). While the A cation is often considered electronically relatively inactive, it significantly affects both SH kinetics and the threshold for photodamage. The SH kinetics are markedly faster for γ-CsPbI3 and α-FAPbI3 than for MAPbI3. Furthermore, γ-CsPbI3 exhibits an intricate interplay between photoinduced darkening and brightening. We suggest possible explanations for the observed differences in SH behavior. This study’s results are essential for identifying absorber materials that can regain intrinsic, insolation-induced photodamage-linked efficiency loss during its rest cycles, thus enabling applications such as autonomously sustainable electronics.

quote

GB/T 7714-2015 [1] Pallavi Singh, Yahel Soffer, Davide Raffaele Ceratti, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00017.
MLA [1] Pallavi Singh, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00017.
APA [1] Pallavi Singh, Yahel Soffer, Davide Raffaele Ceratti, Michael Elbaum, Dan Oron, Gary Hodes, & David Cahen. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00017
IEEE [1] Pallavi Singh, Yahel Soffer, Davide Raffaele Ceratti, Michael Elbaum, Dan Oron, Gary Hodes, and David Cahen, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00017.