Bio-Inspired Self-Cleaning Surfaces AITranslate

beihang university; beihang university
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Self-cleaning surfaces have drawn a lot of interest for both fundamental research and practical applications. This review focuses on the recent progress in mechanism, preparation, and application of self-cleaning surfaces. To date, self-cleaning has been demonstrated by the following four conceptual approaches: (a) TiO2-based superhydrophilic self-cleaning, (b) lotus effect self-cleaning (superhydrophobicity with a small sliding angle), (c) gecko setae–inspired self-cleaning, and (d) underwater organisms–inspired antifouling self-cleaning. Although a number of self-cleaning products have been commercialized, the remaining challenges and future outlook of self-cleaning surfaces are also briefly addressed. Through evolution, nature, which has long been a source of inspiration for scientists and engineers, has arrived at what is optimal. We hope this review will stimulate interdisciplinary collaboration among material science, chemistry, biology, physics, nanoscience, engineering, etc., which is essential for the rational design and reproducible construction of bio-inspired multifunctional self-cleaning surfaces in practical applications.

KeyWords AITranslate

antiicing antifogging antireflection drag reduction superhydrophilicity superhydrophobicity
No data

Basic Information:

DOI:https://doi.org/10.1146/annurev-matsci-070511-155046

Chinese Library Classification Number:

Citation Information:

Self-cleaning surfaces have drawn a lot of interest for both fundamental research and practical applications. This review focuses on the recent progress in mechanism, preparation, and application of self-cleaning surfaces. To date, self-cleaning has been demonstrated by the following four conceptual approaches: (a) TiO2-based superhydrophilic self-cleaning, (b) lotus effect self-cleaning (superhydrophobicity with a small sliding angle), (c) gecko setae–inspired self-cleaning, and (d) underwater organisms–inspired antifouling self-cleaning. Although a number of self-cleaning products have been commercialized, the remaining challenges and future outlook of self-cleaning surfaces are also briefly addressed. Through evolution, nature, which has long been a source of inspiration for scientists and engineers, has arrived at what is optimal. We hope this review will stimulate interdisciplinary collaboration among material science, chemistry, biology, physics, nanoscience, engineering, etc., which is essential for the rational design and reproducible construction of bio-inspired multifunctional self-cleaning surfaces in practical applications.

quote

GB/T 7714-2015 [1] Kesong Liu, Lei Jiang. Annual Review of Materials Research, 2012(42). DOI:10.1146/annurev-matsci-070511-155046.
MLA [1] Kesong Liu, and Lei Jiang. Annual Review of Materials Research, no. 42, 2012, https://doi.org/10.1146/annurev-matsci-070511-155046.
APA [1] Kesong Liu, & Lei Jiang. (2012). Annual Review of Materials Research(42). https://doi.org/10.1146/annurev-matsci-070511-155046
IEEE [1] Kesong Liu and Lei Jiang, Annual Review of Materials Research, no. 42, 2012, doi: 10.1146/annurev-matsci-070511-155046. keywords: {antiicing;antifogging;antireflection;drag reduction;superhydrophilicity;superhydrophobicity}