daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Porous 3D-Biocomposite Adsorbent for Iron Reclamation and Use in Agricultural Applications AITranslate

University of Florida; Central South University of Forestry and Technology; University of Florida; University of Florida; University of Florida; Shandong Agricultural University; Georgia Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The essential nutrients (e.g., iron) for food production are nonrenewable resources, which cannot satisfy the need of a fast-growing global population. Meanwhile, excessive irons accumulated in iron-rich water pose an adverse effect on human and ecosystem health. Thus, it is necessary to develop a cost-effective and eco-friendly adsorbent for reclaiming irons from iron-accumulated water and which cannot satisfy the need of a fast-growing global population. Meanwhile, excessive irons accumulated in iron-rich water pose an adverse effect on human and ecosystem health. Thus, it is necessary to develop a cost-effective and eco-friendly adsorbent for reclaiming irons from iron-accumulated water and these irons for growing crops. In this study, a simple gelation–solidification process aided by phase separation is developed to fabricate a biodegradable alginate/polyvinyl alcohol/lignosulfonate (SA/PVA/LS) three-dimensional (3D) biocomposite adsorbent. Calcium chloride and boric acid are used as cross-linkers between polymers with hydroxyl groups. This bioadsorbent owns a multiporous architecture, ample functional groups, and enhanced total pore volume. A multilayer adsorption mechanism endows it with a high iron adsorption capacity (52 mg/g) via Langmuir simulation and a physiochemical adsorption mechanism. The porous 3D structure of the biocomposite could be observed from SEM and CT scanning. After iron loading, it can be applied as an excellent substitute for a commercial EDTA-Fe micronutrient to promote plant growth with a comparable ratio of root to shoot length. This eco-friendly, highly efficient, and filled 3D bioadsorbent is expected to open a door to achieving circular recovery of plant essential plant nutrients from waste resources for crop production.

KeyWords AITranslate

biopolymer filled 3D biocomposite iron reclaiming multipore adsorbents plant micronutrient
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01198

Chinese Library Classification Number:

Citation Information:

The essential nutrients (e.g., iron) for food production are nonrenewable resources, which cannot satisfy the need of a fast-growing global population. Meanwhile, excessive irons accumulated in iron-rich water pose an adverse effect on human and ecosystem health. Thus, it is necessary to develop a cost-effective and eco-friendly adsorbent for reclaiming irons from iron-accumulated water and which cannot satisfy the need of a fast-growing global population. Meanwhile, excessive irons accumulated in iron-rich water pose an adverse effect on human and ecosystem health. Thus, it is necessary to develop a cost-effective and eco-friendly adsorbent for reclaiming irons from iron-accumulated water and these irons for growing crops. In this study, a simple gelation–solidification process aided by phase separation is developed to fabricate a biodegradable alginate/polyvinyl alcohol/lignosulfonate (SA/PVA/LS) three-dimensional (3D) biocomposite adsorbent. Calcium chloride and boric acid are used as cross-linkers between polymers with hydroxyl groups. This bioadsorbent owns a multiporous architecture, ample functional groups, and enhanced total pore volume. A multilayer adsorption mechanism endows it with a high iron adsorption capacity (52 mg/g) via Langmuir simulation and a physiochemical adsorption mechanism. The porous 3D structure of the biocomposite could be observed from SEM and CT scanning. After iron loading, it can be applied as an excellent substitute for a commercial EDTA-Fe micronutrient to promote plant growth with a comparable ratio of root to shoot length. This eco-friendly, highly efficient, and filled 3D bioadsorbent is expected to open a door to achieving circular recovery of plant essential plant nutrients from waste resources for crop production.

quote

GB/T 7714-2015 [1] Shanyu Meng, Hui Wang, Yuncong C. Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01198.
MLA [1] Shanyu Meng, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01198.
APA [1] Shanyu Meng, Hui Wang, Yuncong C. Li, Tiantian Li, Guodong Liu, Shugang Zhang, & Zhaohui Tong. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01198
IEEE [1] Shanyu Meng, Hui Wang, Yuncong C. Li, Tiantian Li, Guodong Liu, Shugang Zhang, and Zhaohui Tong, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01198. keywords: {biopolymer;filled 3D biocomposite;iron reclaiming;multipore adsorbents;plant micronutrient}