daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Importance of Functional Groups in Cross-Linking Methoxysilane Additives for High-Efficiency and Stable Perovskite Solar Cells AITranslate

Korea|Energy Research Institute @ Nanyang Technological University (NTU) (ERI@N); Sungkyunkwan University; Nanyang Technological University (NTU); Sungkyunkwan University; Sungkyunkwan University; 639798 Singapore|Energy Research Institute @ Nanyang Technological University (NTU) (ERI@N); Sungkyunkwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Here we report an efficient and reproducible multifunctional additive engineering strategy via methoxysilane cross-linking agents functionalized by the different terminal group, moderate electron-donating −SH, weak electron-donating −CH3, or strong electron-withdrawing −CN, into a PbI2 precursor solution. The power conversion efficiency (PCE) is increased from 18.4 to 20.8% after introduction of (3-mercaptopropyl)trimethoxysilane (MPTS) containing a −SH group as a consequence of improved voltage and current density, while 3-cyanopropyltriethoxysilane (CPTS) containing a −CN group deteriorates the overall photovoltaic performance. Moreover, −SH in MPTS is found to passivate defects effectively through a Lewis acid–base interaction with PbI2, resulting in a larger grain size and a longer carrier lifetime. Owing to the formation of a cross-linking siloxane network as a protective layer on the grain boundary, the thermal and moisture stability of the device are improved remarkably. The present work provides a guideline for multifunctional additive engineering for the purpose of simultaneous achievement of a high PCE and long-term stability.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01356

Chinese Library Classification Number:

Citation Information:

Here we report an efficient and reproducible multifunctional additive engineering strategy via methoxysilane cross-linking agents functionalized by the different terminal group, moderate electron-donating −SH, weak electron-donating −CH3, or strong electron-withdrawing −CN, into a PbI2 precursor solution. The power conversion efficiency (PCE) is increased from 18.4 to 20.8% after introduction of (3-mercaptopropyl)trimethoxysilane (MPTS) containing a −SH group as a consequence of improved voltage and current density, while 3-cyanopropyltriethoxysilane (CPTS) containing a −CN group deteriorates the overall photovoltaic performance. Moreover, −SH in MPTS is found to passivate defects effectively through a Lewis acid–base interaction with PbI2, resulting in a larger grain size and a longer carrier lifetime. Owing to the formation of a cross-linking siloxane network as a protective layer on the grain boundary, the thermal and moisture stability of the device are improved remarkably. The present work provides a guideline for multifunctional additive engineering for the purpose of simultaneous achievement of a high PCE and long-term stability.

quote

GB/T 7714-2015 [1] Lin Xie, Jiangzhao Chen, Parth Vashishtha, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01356.
MLA [1] Lin Xie, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01356.