Extremely Stable Sodium Metal Batteries Enabled by Localized High-Concentration Electrolytes AITranslate

Pacific Northwest National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sodium (Na) metal is a promising anode for Na-ion batteries. However, the high reactivity of Na metal with electrolytes and the low Na metal cycling efficiency have limited its practical application in rechargeable Na metal batteries. High-concentration electrolytes (HCE, ≥4 M) consisting of sodium bis(fluorosulfonyl)imide (NaFSI) and ether solvent could ensure the stable cycling of Na metal with high Coulombic efficiency but at the cost of high viscosity, poor wettability, and high salt cost. Here, we report that the salt concentration could be significantly reduced (≤1.5 M) by a hydrofluoroether as an “inert” diluent, which maintains the solvation structures of HCE, thereby forming a localized high-concentration electrolyte (LHCE). A LHCE [2.1 M NaFSI/1,2-dimethoxyethane (DME)–bis(2,2,2-trifluoroethyl) ether (BTFE) (solvent molar ratio 1:2)] enables dendrite-free Na deposition with a high Coulombic efficiency of >99%, fast charging (20C), and stable cycling (90.8% retention after 40 000 cycles) of Na∥Na3V2(PO4)3 batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01213

Chinese Library Classification Number:

Citation Information:

Sodium (Na) metal is a promising anode for Na-ion batteries. However, the high reactivity of Na metal with electrolytes and the low Na metal cycling efficiency have limited its practical application in rechargeable Na metal batteries. High-concentration electrolytes (HCE, ≥4 M) consisting of sodium bis(fluorosulfonyl)imide (NaFSI) and ether solvent could ensure the stable cycling of Na metal with high Coulombic efficiency but at the cost of high viscosity, poor wettability, and high salt cost. Here, we report that the salt concentration could be significantly reduced (≤1.5 M) by a hydrofluoroether as an “inert” diluent, which maintains the solvation structures of HCE, thereby forming a localized high-concentration electrolyte (LHCE). A LHCE [2.1 M NaFSI/1,2-dimethoxyethane (DME)–bis(2,2,2-trifluoroethyl) ether (BTFE) (solvent molar ratio 1:2)] enables dendrite-free Na deposition with a high Coulombic efficiency of >99%, fast charging (20C), and stable cycling (90.8% retention after 40 000 cycles) of Na∥Na3V2(PO4)3 batteries.

quote

GB/T 7714-2015 [1] JiGuang Zhang. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01213.
MLA [1] JiGuang Zhang. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01213.
APA [1] JiGuang Zhang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01213
IEEE [1] JiGuang Zhang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01213.