Could Nanocomposites Continue the Success of Halide Perovskites? AITranslate
Abstract AITranslate
Halide perovskites have shown great potential for next-generation optoelectronics. Despite the high efficiency of devices achieved in the laboratory, instability in long-term device operation stalls commercialization. A particular concern is how the remarkable physical properties can be retained when the photoactive materials are integrated into functional devices. Although not prevailing yet, creating nanocomposites of halide perovskites has shown promise to solve some of the instability issues in the initial work. In this Perspective, we discuss the advantages, current limitations, and challenges of perovskite composites and their effects on the physical properties. In order to provide an outlook of future directions, we also highlight some open questions related to carrier dynamics, interfacial effects, and charge transport properties.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00580
Chinese Library Classification Number:
Citation Information:
Halide perovskites have shown great potential for next-generation optoelectronics. Despite the high efficiency of devices achieved in the laboratory, instability in long-term device operation stalls commercialization. A particular concern is how the remarkable physical properties can be retained when the photoactive materials are integrated into functional devices. Although not prevailing yet, creating nanocomposites of halide perovskites has shown promise to solve some of the instability issues in the initial work. In this Perspective, we discuss the advantages, current limitations, and challenges of perovskite composites and their effects on the physical properties. In order to provide an outlook of future directions, we also highlight some open questions related to carrier dynamics, interfacial effects, and charge transport properties.
quote
| GB/T 7714-2015 | [1] Xi Wang, Xiujun Lian, Zihan Zhang, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00580. |
| MLA | [1] Xi Wang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00580. |
| APA | [1] Xi Wang, Xiujun Lian, Zihan Zhang, & Hanwei Gao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00580 |
| IEEE | [1] Xi Wang, Xiujun Lian, Zihan Zhang, and Hanwei Gao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00580. |