Carbon Confined Mesoporous Catkin-like SnPS3 Nanostructure for Lithium Storage with Great Superiority AITranslate

Harbin Engineering University; Harbin Engineering University;BTR New Energy Materials, Inc.; Harbin Engineering University; Central South University; Naval University of Engineering;Wuhan Second Ship Design and Research Institute; Harbin Engineering University; Harbin Engineering University; Peking University; Harbin Engineering University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal phosphosulfides (MPSs) are members of a category of emerging energy storage and conversion materials, particularly having significant potentials in lithium storage due to their phosphorus and sulfur dual anion centers and unique two-dimensional channels. Nevertheless, it is still very challenging for the controllable design and synthesis of MPSs nanomaterials with complex-element components. Herein, a distinctive carbon confined mesoporous catkin-like SnPS3 nanostructure (SnPS3@C) is controllably synthesized and fabricated based on the partial volatilization of the reduced tin and the following bottom-up phosphosulfuration by a chemical vapor deposition method. As the anode material of lithium ion batteries, the catkin-like SnPS3@C offers multiple active centers for lithium insertion, complete carbon shell to protect inner active materials, interlaced fibrous networks for efficient electron transfer as well as abundant inner mesopores for Li+ diffusion and volume buffer, thus showing prominent structure advantages in lithium storage. The catkin-like SnPS3@C electrode demonstrated superior electrochemical capability with a very high reversible capacity (1302 mAh g–1 at 300 mA g–1), excellent rate property (630 mAh g–1 at 8000 mA g–1) and distinguished cycling stability (1030 mAh g–1 after 1000 cycles at 1000 mA g–1). This work offers a new avenue to develop high-performance MPSs materials for advanced lithium ion batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00011

Chinese Library Classification Number:

Citation Information:

Metal phosphosulfides (MPSs) are members of a category of emerging energy storage and conversion materials, particularly having significant potentials in lithium storage due to their phosphorus and sulfur dual anion centers and unique two-dimensional channels. Nevertheless, it is still very challenging for the controllable design and synthesis of MPSs nanomaterials with complex-element components. Herein, a distinctive carbon confined mesoporous catkin-like SnPS3 nanostructure (SnPS3@C) is controllably synthesized and fabricated based on the partial volatilization of the reduced tin and the following bottom-up phosphosulfuration by a chemical vapor deposition method. As the anode material of lithium ion batteries, the catkin-like SnPS3@C offers multiple active centers for lithium insertion, complete carbon shell to protect inner active materials, interlaced fibrous networks for efficient electron transfer as well as abundant inner mesopores for Li+ diffusion and volume buffer, thus showing prominent structure advantages in lithium storage. The catkin-like SnPS3@C electrode demonstrated superior electrochemical capability with a very high reversible capacity (1302 mAh g–1 at 300 mA g–1), excellent rate property (630 mAh g–1 at 8000 mA g–1) and distinguished cycling stability (1030 mAh g–1 after 1000 cycles at 1000 mA g–1). This work offers a new avenue to develop high-performance MPSs materials for advanced lithium ion batteries.

quote

GB/T 7714-2015 [1] Gaofu Li, Xianglong Kong, Lei Chen, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00011.
MLA [1] Gaofu Li, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00011.
APA [1] Gaofu Li, Xianglong Kong, Lei Chen, Liu Liu, Xinghua Chang, Xiangxi Wang, Qingjie Meng, Fei He, Piaoping Yang, Jie Zheng, & Zhiliang Liu. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00011
IEEE [1] Gaofu Li, Xianglong Kong, Lei Chen, Liu Liu, Xinghua Chang, Xiangxi Wang, Qingjie Meng, Fei He, Piaoping Yang, Jie Zheng, and Zhiliang Liu, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00011.