Experimental investigation and thermodynamic modeling of the Cu–Mn–Ni system AITranslate
Abstract AITranslate
The phase equilibria of the ternary Cu–Mn–Ni system in the region above 40 at.% Mn at 600 ∘C were investigated by means of optical microscopy, X-ray diffraction, scanning electron microscopy with energy dispersive X-ray spectroscopy and electron probe microanalysis. The isothermal section of the Cu–Mn–Ni system at 600 ∘C consists of 4 two-phase regions (cbcc_A12 +fcc_A1, cub_A13 +fcc_A1, cbcc_A12 + cub_A13, L 1 0 +fcc_A1) and 1 three-phase region (cbcc_A12 +cub_A13 +fcc_A1). The disordered fcc_A1 phase exhibits a large continuous solution between γ (Cu,Ni) and γ (Mn). The L 1 0 phase only equilibrates with fcc_A1 phase, and the solubility of Cu in L 1 0 phase is up to 16 at.%. A thermodynamic modeling for this system was performed by considering reliable literature data and incorporating the current experimental results. A self-consistent set of thermodynamic parameters was obtained, and the calculated results show a general agreement with the experimental data.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2009.07.003
Chinese Library Classification Number:
Citation Information:
The phase equilibria of the ternary Cu–Mn–Ni system in the region above 40 at.% Mn at 600 ∘C were investigated by means of optical microscopy, X-ray diffraction, scanning electron microscopy with energy dispersive X-ray spectroscopy and electron probe microanalysis. The isothermal section of the Cu–Mn–Ni system at 600 ∘C consists of 4 two-phase regions (cbcc_A12 +fcc_A1, cub_A13 +fcc_A1, cbcc_A12 + cub_A13, L 1 0 +fcc_A1) and 1 three-phase region (cbcc_A12 +cub_A13 +fcc_A1). The disordered fcc_A1 phase exhibits a large continuous solution between γ (Cu,Ni) and γ (Mn). The L 1 0 phase only equilibrates with fcc_A1 phase, and the solubility of Cu in L 1 0 phase is up to 16 at.%. A thermodynamic modeling for this system was performed by considering reliable literature data and incorporating the current experimental results. A self-consistent set of thermodynamic parameters was obtained, and the calculated results show a general agreement with the experimental data.
quote
| GB/T 7714-2015 | [1] WeiHua Sun, HongHui Xu, Yong Du, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.07.003. |
| MLA | [1] WeiHua Sun, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.07.003. |
| APA | [1] WeiHua Sun, HongHui Xu, Yong Du, ShuHong Liu, HaiLin Chen, LiJun Zhang, & BaiYun Huang. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2009.07.003 |
| IEEE | [1] WeiHua Sun, HongHui Xu, Yong Du, ShuHong Liu, HaiLin Chen, LiJun Zhang, and BaiYun Huang, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2009.07.003. |