Metal-Free, Low-Surface Energy, and Self-Healing Polyurethane Coating with an Excellent Antifouling Property AITranslate

Suzhou University of Science and Technology; Suzhou University of Science and Technology; Suzhou University of Science and Technology; Suzhou University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The prevention and control of water biofouling has always been the focus of antifouling research. Coatings containing metal ions can effectively inhibit biofouling. However, the application of this type of coating has been limited as a result of its toxicity, irreparability, and poor antifouling ability under static conditions. Here, we have synthesized a self-repairing polymer antifouling coating with hydrophobic and multiple self-repairing systems through structural design with polytetrahydrofuran (PTMEG), isophorone diisocyanate (IPDI), perfluorooctyl ethyl acrylate (TEAc-8), triclosan (TCS), and 3,3-dithiodipropionic acid as a raw material. The prepared coating can realize a self-repairing function at room temperature in both air and water, thereby prolonging the antifouling life of the coating. A large number of hydrogen bonds in the molecular structure enable the coating to have good adhesion to the substrate. At the same time, the lower surface energy (<20 mN/m) and higher hydrophobic angle (>110°) of the coating determine the material’s good fouling release ability. In addition, the lake antifouling experiments show that the coating has good static antifouling ability. The coatings prepared will provide an alternative strategy for designing self-healing marine antifouling coatings in practical applications.

KeyWords AITranslate

environmentally friendly polyurethane fouling release fouling resistance selfhealing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01503

Chinese Library Classification Number:

Citation Information:

The prevention and control of water biofouling has always been the focus of antifouling research. Coatings containing metal ions can effectively inhibit biofouling. However, the application of this type of coating has been limited as a result of its toxicity, irreparability, and poor antifouling ability under static conditions. Here, we have synthesized a self-repairing polymer antifouling coating with hydrophobic and multiple self-repairing systems through structural design with polytetrahydrofuran (PTMEG), isophorone diisocyanate (IPDI), perfluorooctyl ethyl acrylate (TEAc-8), triclosan (TCS), and 3,3-dithiodipropionic acid as a raw material. The prepared coating can realize a self-repairing function at room temperature in both air and water, thereby prolonging the antifouling life of the coating. A large number of hydrogen bonds in the molecular structure enable the coating to have good adhesion to the substrate. At the same time, the lower surface energy (<20 mN/m) and higher hydrophobic angle (>110°) of the coating determine the material’s good fouling release ability. In addition, the lake antifouling experiments show that the coating has good static antifouling ability. The coatings prepared will provide an alternative strategy for designing self-healing marine antifouling coatings in practical applications.

quote

GB/T 7714-2015 [1] Rijia Jiang, Mengyue Liu, Xiangyu Zheng, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01503.
MLA [1] Rijia Jiang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01503.
APA [1] Rijia Jiang, Mengyue Liu, Xiangyu Zheng, & Xing Zhou. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01503
IEEE [1] Rijia Jiang, Mengyue Liu, Xiangyu Zheng, and Xing Zhou, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01503. keywords: {environmentally friendly;polyurethane;fouling release;fouling resistance;selfhealing}