Effect of Temperature and Hydrophilic Ratio on the Structure of Poly(N-vinylcaprolactam)-block-poly(dimethylsiloxane)-block-poly(N-vinylcaprolactam) Polymersomes AITranslate

University of Alabama at Birmingham; University of Alabama at Birmingham; University of Alabama at Birmingham; University of Illinois at Urbana−Champaign; University of Illinois at Urbana−Champaign; Construction Engineering Research Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Construction Engineering Research Laboratory; University of Illinois at Urbana−Champaign; University of Alabama at Birmingham
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nanosized polymeric vesicles (polymersomes) assembled from ABA triblock copolymers of poly(N-vinylcaprolactam)-poly(dimethylsiloxane)-poly(N-vinylcaprolactam) (PVCL–PDMS–PVCL) are a promising platform for biomedical applications, as the temperature-responsiveness of the PVCL blocks enables reversible vesicle shrinkage and permeability of the polymersome shell at elevated temperatures. Herein, we explore the effects of molecular weight, polymer block weight ratios, and temperature on the structure of these polymersomes via electron microscopy, dynamic light scattering, small angle neutron scattering (SANS), and all-atom molecular dynamics methods. We show that the shell structure and overall size of the polymersome can be tuned by varying the hydrophilic (PVCL) weight fraction of the polymer: at room temperature, polymers of smaller hydrophilic ratios form larger vesicles that have thinner shells, whereas polymers with higher PVCL content exhibit interchain aggregation of PVCL blocks within the polymersome shell above 50 °C. Model fitting and model-free analysis of the SANS data reveals that increasing the mass ratio of PVCL to the total copolymer weight from 0.3 to 0.56 reduces the temperature-induced change in vesicle diameter by a factor of 3, while simultaneously increasing the change in shell thickness by a factor of 1.5. Finally, by analysis of the shell structures and overall size of polymersomes with various PVCL weight ratios and those without temperature-dependent polymer components, we bring into focus the mechanism of temperature-triggered drug release reported in a previous study. This work provides new fundamental perspectives on temperature-responsive polymersomes and elucidates important structure–property relationships of their constituent polymers.

KeyWords AITranslate

polymersomes temperature responsive SANS molecular dynamics poly(Nvinylcaprolactam) triblock copolymer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00259

Chinese Library Classification Number:

Citation Information:

Nanosized polymeric vesicles (polymersomes) assembled from ABA triblock copolymers of poly(N-vinylcaprolactam)-poly(dimethylsiloxane)-poly(N-vinylcaprolactam) (PVCL–PDMS–PVCL) are a promising platform for biomedical applications, as the temperature-responsiveness of the PVCL blocks enables reversible vesicle shrinkage and permeability of the polymersome shell at elevated temperatures. Herein, we explore the effects of molecular weight, polymer block weight ratios, and temperature on the structure of these polymersomes via electron microscopy, dynamic light scattering, small angle neutron scattering (SANS), and all-atom molecular dynamics methods. We show that the shell structure and overall size of the polymersome can be tuned by varying the hydrophilic (PVCL) weight fraction of the polymer: at room temperature, polymers of smaller hydrophilic ratios form larger vesicles that have thinner shells, whereas polymers with higher PVCL content exhibit interchain aggregation of PVCL blocks within the polymersome shell above 50 °C. Model fitting and model-free analysis of the SANS data reveals that increasing the mass ratio of PVCL to the total copolymer weight from 0.3 to 0.56 reduces the temperature-induced change in vesicle diameter by a factor of 3, while simultaneously increasing the change in shell thickness by a factor of 1.5. Finally, by analysis of the shell structures and overall size of polymersomes with various PVCL weight ratios and those without temperature-dependent polymer components, we bring into focus the mechanism of temperature-triggered drug release reported in a previous study. This work provides new fundamental perspectives on temperature-responsive polymersomes and elucidates important structure–property relationships of their constituent polymers.

quote

GB/T 7714-2015 [1] Yiming Yang, Aaron Alford, Veronika Kozlovskaya, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00259.
MLA [1] Yiming Yang, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00259.
APA [1] Yiming Yang, Aaron Alford, Veronika Kozlovskaya, Shidi Zhao, Himanshu Joshi, Eunjung Kim, Shuo Qian, Volker Urban, Donald Cropek, Aleksei Aksimentiev, & Eugenia Kharlampieva. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00259
IEEE [1] Yiming Yang, Aaron Alford, Veronika Kozlovskaya, Shidi Zhao, Himanshu Joshi, Eunjung Kim, Shuo Qian, Volker Urban, Donald Cropek, Aleksei Aksimentiev, and Eugenia Kharlampieva, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00259. keywords: {polymersomes;temperature responsive;SANS;molecular dynamics;poly(Nvinylcaprolactam);triblock copolymer}