daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hydrogen-Bond-Assisted Dye-Incorporated Waterborne Poly( urethane-urea) (WPU) for an Environment-Friendly Textile Dyeing Process AITranslate

National Taipei University of Technology; National Taipei University of Technology; National Taipei University of Technology; National Taipei University of Technology; National Taipei University of Technology; National Taipei University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To propose a green dyeing strategy permitting the incorporation of chromophores via the promotion of physical bonding and a simple sewage processing procedure, a strategy for increasing the reactivity of a conventional disperse dye, namely, 1-amino-4-hydroxy-2-phenoxyanthraquinone (Disperse Red 60, R60), to isocyanate groups and miscibility with waterborne poly(urethane-urea) (WPU) was reported. The modified dye R60-OH was prepared by the alkylation of 3-bromopropan-1-ol. Subsequently, R60-OH was reacted with the trifunctional isocyanate (named R60-O-THDI), which provided additional hydrogen bonds between the dye and the polymer chain and rendered better color fastness. Polyester, nylon, and cotton fabric coated with R60 and R60-O-THDI-incorporated WPUs were investigated by colorimetric analysis, washing tests, and rubbing color fastness. R60-O-THDI exhibited the best rubbing and washing color fastness, indicative of a simple method to fabricate a water-based dye ink without grafting a chromophore onto a polymer backbone via the promotion of physical bonding. The proposed green dyeing strategy also permitted a simple sewage processing procedure to recover polyurethane from the suspension by changing the pH, rendering better color fastness on textiles, as well as less wastewater production.

KeyWords AITranslate

waterborne polyurethane (WPU) disperse dye textile green dye
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02238

Chinese Library Classification Number:

Citation Information:

To propose a green dyeing strategy permitting the incorporation of chromophores via the promotion of physical bonding and a simple sewage processing procedure, a strategy for increasing the reactivity of a conventional disperse dye, namely, 1-amino-4-hydroxy-2-phenoxyanthraquinone (Disperse Red 60, R60), to isocyanate groups and miscibility with waterborne poly(urethane-urea) (WPU) was reported. The modified dye R60-OH was prepared by the alkylation of 3-bromopropan-1-ol. Subsequently, R60-OH was reacted with the trifunctional isocyanate (named R60-O-THDI), which provided additional hydrogen bonds between the dye and the polymer chain and rendered better color fastness. Polyester, nylon, and cotton fabric coated with R60 and R60-O-THDI-incorporated WPUs were investigated by colorimetric analysis, washing tests, and rubbing color fastness. R60-O-THDI exhibited the best rubbing and washing color fastness, indicative of a simple method to fabricate a water-based dye ink without grafting a chromophore onto a polymer backbone via the promotion of physical bonding. The proposed green dyeing strategy also permitted a simple sewage processing procedure to recover polyurethane from the suspension by changing the pH, rendering better color fastness on textiles, as well as less wastewater production.

quote

GB/T 7714-2015 [1] ShuYi Chen, ShangJu Lu, Yen Ju Cuo, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02238.
MLA [1] ShuYi Chen, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02238.