Main Chain 1,5-Disubstituted-1H-Tetrazole-Based Polymers via Ugi-Azide-Four-Multicomponent Polymerization (UA-4MCP) AITranslate

Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); Universidad Nacional de San Martín (INS-UNSAM); UMR 7361 CNRS/Université de Haute Alsace; Karlsruhe Institute of Technology (KIT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The utilization of the distinctive molecular architecture of tetrazoles, which comprises a five-membered ring containing four nitrogen atoms, offers tremendous potential in the field of polymer chemistry. Although research on pendant chain tetrazole-containing polymers has been considerably reported, the exploration of advanced synthesis methods for main chain tetrazole-based polymers has not been extensively undertaken. On this premise, the synthesis of main chain 1,5-disubstituted-1H-tetrazole (1,5-DS-T)-based compounds was investigated to showcase the possibility of polymer formation by using the Ugi-azide-four-multicomponent polymerization (UA-4MCP) strategy. Particularly, UA-4MC polymers were designed with various side groups (e.g., aliphatic or aromatic) and engineered for a post-polymerization modification via thiol-ene photo-click reaction. The chemical characterization confirmed 1,5-DS-T-based polymer formation with a number average molecular mass (Mn) up to 8500 g mol–1. Importantly, side-group variation permitted tuning the glass-transition temperature (Tg) between −25 and 60 °C. Furthermore, the polymers exhibited moderate thermal stability up to 305 ± 10 °C besides interesting nonconventional fluorescence behavior.

KeyWords AITranslate

nitrogen heterocycles 1 5disubstitutedtetrazole multicomponent reaction thiolene photoclick reaction heteroatom Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01231

Chinese Library Classification Number:

Citation Information:

The utilization of the distinctive molecular architecture of tetrazoles, which comprises a five-membered ring containing four nitrogen atoms, offers tremendous potential in the field of polymer chemistry. Although research on pendant chain tetrazole-containing polymers has been considerably reported, the exploration of advanced synthesis methods for main chain tetrazole-based polymers has not been extensively undertaken. On this premise, the synthesis of main chain 1,5-disubstituted-1H-tetrazole (1,5-DS-T)-based compounds was investigated to showcase the possibility of polymer formation by using the Ugi-azide-four-multicomponent polymerization (UA-4MCP) strategy. Particularly, UA-4MC polymers were designed with various side groups (e.g., aliphatic or aromatic) and engineered for a post-polymerization modification via thiol-ene photo-click reaction. The chemical characterization confirmed 1,5-DS-T-based polymer formation with a number average molecular mass (Mn) up to 8500 g mol–1. Importantly, side-group variation permitted tuning the glass-transition temperature (Tg) between −25 and 60 °C. Furthermore, the polymers exhibited moderate thermal stability up to 305 ± 10 °C besides interesting nonconventional fluorescence behavior.

quote

GB/T 7714-2015 [1] Meryem S. Akdemir, Birgit Huber, Marina Simian, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01231.
MLA [1] Meryem S. Akdemir, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01231.
APA [1] Meryem S. Akdemir, Birgit Huber, Marina Simian, Hatice Mutlu, & Patrick Theato. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01231
IEEE [1] Meryem S. Akdemir, Birgit Huber, Marina Simian, Hatice Mutlu, and Patrick Theato, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01231. keywords: {nitrogen heterocycles;1;5disubstitutedtetrazole;multicomponent reaction;thiolene photoclick reaction;heteroatom;Show More}