daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Spectrally Selective Polarization-Sensitive Photodetection Based on a 1D Lead-Free Hybrid Perovskite Ferroelectric AITranslate

Southeast University; Southeast University; Southeast University; Southeast University; Southeast University; Southeast University; Southeast University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Green, self-powered, flexible, and tunable features have been greatly desired to satisfy the increasing demands for next-generation photodetectors and sensors. Here, we report a 1D lead-free perovskite ferroelectric HDA-BiI5 (HDA = hexane-1,6-diammonium) based photodetector showing a spectrally selective linear polarized light response due to a unique linear dichroic conversion behavior. The HDA-BiI5 single crystal device shows an orthogonal reverse of polarization-sensitive photocurrent and can distinguish linearly polarized light in different wavelength ranges with the photocurrent anisotropy ratio ω of about 1.37 at 405 nm, 1.00 at 490 nm, and 1.17 at 530 nm. Importantly, the device achieves a ferroelectricity-driven self-powered detection with an excellent ω (∼1.28 at 405 nm) and a high detectivity D* of 5.3 × 108 Jones. This research provides a pathway for the design of future integratable polarization-sensitive photodetectors.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00539

Chinese Library Classification Number:

Citation Information:

Green, self-powered, flexible, and tunable features have been greatly desired to satisfy the increasing demands for next-generation photodetectors and sensors. Here, we report a 1D lead-free perovskite ferroelectric HDA-BiI5 (HDA = hexane-1,6-diammonium) based photodetector showing a spectrally selective linear polarized light response due to a unique linear dichroic conversion behavior. The HDA-BiI5 single crystal device shows an orthogonal reverse of polarization-sensitive photocurrent and can distinguish linearly polarized light in different wavelength ranges with the photocurrent anisotropy ratio ω of about 1.37 at 405 nm, 1.00 at 490 nm, and 1.17 at 530 nm. Importantly, the device achieves a ferroelectricity-driven self-powered detection with an excellent ω (∼1.28 at 405 nm) and a high detectivity D* of 5.3 × 108 Jones. This research provides a pathway for the design of future integratable polarization-sensitive photodetectors.

quote

GB/T 7714-2015 [1] ChengDong Liu, ChangChun Fan, BeiDou Liang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00539.
MLA [1] ChengDong Liu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00539.
APA [1] ChengDong Liu, ChangChun Fan, BeiDou Liang, ChaoYang Chai, ChangQing Jing, XiangBin Han, & Wen Zhang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00539
IEEE [1] ChengDong Liu, ChangChun Fan, BeiDou Liang, ChaoYang Chai, ChangQing Jing, XiangBin Han, and Wen Zhang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00539.