Abstract AITranslate

The experimental measurement of the evolution of interfaces in three dimensions is reviewed, concentrating on the evolution of polycrystalline and solid-liquid systems, including growth and coarsening in dendritic systems and evolution during liquid-phase sintering. Both ex situ destructive techniques and in situ nondestructive techniques are considered. The importance of making three-dimensional measurements that can be quantified and unambiguously compared with theory is discussed, showing that these measurements provide a direct validation of theory and critical initial conditions for simulations.

KeyWords AITranslate

grain growth dendritic coarsening serial sectioning Xray tomography
No data

Basic Information:

DOI:https://doi.org/10.1146/annurev-matsci-070511-155028

Chinese Library Classification Number:

Citation Information:

The experimental measurement of the evolution of interfaces in three dimensions is reviewed, concentrating on the evolution of polycrystalline and solid-liquid systems, including growth and coarsening in dendritic systems and evolution during liquid-phase sintering. Both ex situ destructive techniques and in situ nondestructive techniques are considered. The importance of making three-dimensional measurements that can be quantified and unambiguously compared with theory is discussed, showing that these measurements provide a direct validation of theory and critical initial conditions for simulations.

quote

GB/T 7714-2015 [1] D.J. Rowenhorst, P.W. Voorhees. Annual Review of Materials Research, 2012(42). DOI:10.1146/annurev-matsci-070511-155028.
MLA [1] D.J. Rowenhorst, and P.W. Voorhees. Annual Review of Materials Research, no. 42, 2012, https://doi.org/10.1146/annurev-matsci-070511-155028.
APA [1] D.J. Rowenhorst, & P.W. Voorhees. (2012). Annual Review of Materials Research(42). https://doi.org/10.1146/annurev-matsci-070511-155028
IEEE [1] D.J. Rowenhorst and P.W. Voorhees, Annual Review of Materials Research, no. 42, 2012, doi: 10.1146/annurev-matsci-070511-155028. keywords: {grain growth;dendritic coarsening;serial sectioning;Xray tomography}