Soft Tunable Gelatin Robot with Insect-like Claw for Grasping, Transportation, and Delivery AITranslate

City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; Shenzhen Institutes of Advanced Technology; China|Shenzhen Research Institute of City University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recently, insect-scale soft robots have received increasing attentions for diverse applications owing to their ability to access hard-to-reach areas. However, most of them are composed of non-degradable materials like PDMS and silicone rubbers, and such chemical inertness may become an obstacle for future clinical applications where tunable material properties or degradation abilities are required. Here, we present a small-scale soft robot from a magnetic gelatin hydrogel, whose mechanical properties can be easily tuned through one-step Hofmeister effected-assisted reaction. Moreover, the robot is designed with insect claw-like legged structure, allowing it to perform grasping and cargo transportation tasks as its non-degradable counterparts. The degradation and controlled delivery ability of the robot are also demonstrated to show the advantages of magnetic hydrogels over non-degradable polymers. Our study provides an alternative for the tunable and degradable millirobot construction with an effective manipulation ability and promotes the applications of millirobot in biomedical sceneries.

KeyWords AITranslate

hydrogelbased robots magnetic actuation soft robots bioinspired tunable
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00522

Chinese Library Classification Number:

Citation Information:

Recently, insect-scale soft robots have received increasing attentions for diverse applications owing to their ability to access hard-to-reach areas. However, most of them are composed of non-degradable materials like PDMS and silicone rubbers, and such chemical inertness may become an obstacle for future clinical applications where tunable material properties or degradation abilities are required. Here, we present a small-scale soft robot from a magnetic gelatin hydrogel, whose mechanical properties can be easily tuned through one-step Hofmeister effected-assisted reaction. Moreover, the robot is designed with insect claw-like legged structure, allowing it to perform grasping and cargo transportation tasks as its non-degradable counterparts. The degradation and controlled delivery ability of the robot are also demonstrated to show the advantages of magnetic hydrogels over non-degradable polymers. Our study provides an alternative for the tunable and degradable millirobot construction with an effective manipulation ability and promotes the applications of millirobot in biomedical sceneries.

quote

GB/T 7714-2015 [1] Liu Yang, Jiaqi Miao, Gen Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00522.
MLA [1] Liu Yang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00522.
APA [1] Liu Yang, Jiaqi Miao, Gen Li, Hao Ren, Tieshan Zhang, Dong Guo, Yifeng Tang, Wanfeng Shang, & Yajing Shen. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00522
IEEE [1] Liu Yang, Jiaqi Miao, Gen Li, Hao Ren, Tieshan Zhang, Dong Guo, Yifeng Tang, Wanfeng Shang, and Yajing Shen, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00522. keywords: {hydrogelbased robots;magnetic actuation;soft robots;bioinspired;tunable}